Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brittleness Temperature = -112 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
SABIC FI1157 Bimodal High Density Polyethylene for Blown Film
Product Description: FI1157 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® FF 35 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FF 35 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. The resin shows good strechability and sealability.Main Applications: Greenflex FF 35 is suitable for flexibl..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® FL 25 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FL 25 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FL 25 show good optical properties and excellent sealability.Main Applications: ..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® MH 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion
Greenflex MH 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Items produced with Greenflex MH 40 show high elasticity and good mechanical properties.Main Applic..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® ML 20 Ethylene Vinyl Acetate Copolymer - Injection Molding
Greenflex ML 20 is an ethylene vinyl acetate copolymer (EVA) for injection molding, when a good ESCR is required.Main Applications: Greenflex ML 20 is recommended for the production of flexible ite..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® ML 30 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion
Greenflex ML 30 is an ethylene vinyl acetate copolymer (EVA) for injection molding and profile extrusion. Items produced with Greenflex ML 30 show good ESCR and elasticity.Main Applications: Green..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® ML 31 Ethylene Vinyl Acetate Copolymer - Injection Molding & Profile Extrusion
Greenflex ML 31 is an ethylene vinyl acetate copolymer (EVA) for injection molding applications and extrusion profile. Greenflex ML 31 contains additive waxes to obtain high production speed.Main A..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® ML 40 Ethylene Vinyl Acetate Copolymer - Injection Molding
Greenflex ML 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding of flexible items. Items produced with Greenflex ML 40 show high elasticity and flexibility.Main Applications: Gr..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® ML 60 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion
Greenflex ML 60 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 60 show very high elasticity.Main Applications: Gree..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® MP 35 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion
Greenflex MP 35 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Greenflex MP 35 is an easy flowing material and provides a very high elasticity.Main Applications: ..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® MQ 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding
Greenflex MQ 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MQ 40 combines high fluidity and high elasticity.Main Applications: Green..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® FD 23 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 23 is an ethylene vinyl acetate copolymer (EVA) suitable for blown film extrusion. Greenflex FD 23 is a version of Greenflex FD 20 with added slip and antiblocking agents. Films produ..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® FD 50 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 50 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FD 50 exhibit good optical and sealing properties, high flexibility and toughnes..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Polimeri Europa Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 53 is an ethylene vinyl acetate copolymer (EVA), containing antiblocking agent, for blown film extrusion. Films produced with Greenflex FD 53 exhibit good sealing properties, high flex..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Chevron Phillips Marlex® HMN 55180 High Density Polyethylene  (discontinued **)
High Density PolyethyleneCustomer Benefits: This resin is a narrow molecular weight distribution copolymer with easy processing characteristics and excellent toughness properties. This product disp..
Brittleness Temperature -80.0 °C
-112 °F
ASTM D746
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with No Plasticizer
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Brittleness Temperature -80.0 - -59.0 °C
-112 - -74.2 °F
Average value: -70.8 °C Grade Count:21
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
Brittleness Temperature -80.0 °C
-112 °F
ASTM D746
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, DAM
Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by G..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
LG Chemical LUTENE-H XL1800 HDPE
Description: LUTENE-H XL 1800 is a optimum materials for under-floor heating and drinking water pipe by RAM type extrusion. It is excellent product with long-term internal pressure creep property an..
Brittleness Temperature >= -80.0 °C
>= -112 °F
ASTM D746-72
Iran Petrochemical (PCC) BL 4M HM 8355 High Density Polyethylene
BL4M is a high density polyethylene with 1-Butene as co monomer. It is high molar mass, easily processable, high stiffness and strength, good SCR, very good molding surface finish.Applications: jer..
Brittleness Temperature >= -80.0 °C
>= -112 °F
ASTM D746-72
Iran Petrochemical (PCC) BL2 HF 4750 High Density Polyethylene
BL2 is a high density polyethylene with 1-Butene as co monomer. It is high impact strength and slightly, lower stiffness than BL3, outstanding resistance to stress cracking, even in contact with su..
Brittleness Temperature >= -80.0 °C
>= -112 °F
ASTM D746-72
Iran Petrochemical (PCC) EX 2 S HF 7750 M2 High Density Polyethylene
EX2S is a high density polyethylene with 1-Butene as co monomer. It is medium molar mass, low density grade with a narrow molar mass distribution, high rigidity, good tear strength. Applications: ..
Brittleness Temperature >= -80.0 °C
>= -112 °F
ASTM D746-72
Iran Petrochemical (PCC) EX 5 HM 9450 F High Density Polyethylene
EX5 is a high density polyethylene with 1-Butene as co monomer.Applications: film extrusion, counter bag, carrier bag, wrapping filmsInformation provided by Iran Petrochemical Commercial Co.
Brittleness Temperature >= -80.0 °C
>= -112 °F
ASTM D746-72
Iran Petrochemical (PCC) BL 3VD HH 4765 High Density Polyethylene
BL3VD is a high density polyethylene with 1-Butene as co monomer. It is very high density and stiffness, good ESCR, high flowability and impact strength.Applications: small blow molding, bottles, c..
Brittleness Temperature >= -80.0 °C
>= -112 °F
ASTM D746-72
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene
EX 4HS is a high density polyethylene with 1-Butene as co monomer. It has high rigidity, low gel level, high drawdown, very high stiffness and good tenacity.Applications: film extrusion, blending ..
Brittleness Temperature -80.0 °C
-112 °F
ASTM D746-95
Saint-Gobain Versilicâ„¢ SPX-70I.B. High Strength Silicone Pressure Tubing Formulation
Description: Versilicâ„¢ SPX-70 I.B.: Produced form a proprietary combination of silicone elastomers, Versilicâ„¢ SPX-70 I.B. Tubing optimizes critical physical properties such as tensile st..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Borealis Borcoat™ ME0433 Polyethylene Adhesive In Powder form for Steel Pipe Coating
Borcoat ME0433 is a maleic-anhydride grafted polyethylene polymer with excellent adhesion to fusion bonded epoxy and the top-coat HDPE.Borcoat HE0433 is primarily designed to be used as the tie laye..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;..
Brittleness Temperature -80.0 °C
-112 °F
ASTM D746
Total HDPE 6280 High Density Polyethylene, Injection Molding Resin
Characteristics:Excellent stiffnessExcellent surface appearanceGood warp resistanceExcellent impact resistanceASTM D 1248 - Type III, Class A, Category 3FDA CompliantApplications:Dairy cratesPallets..
Brittleness Temperature <= -80.0 °C
<= -112 °F
ASTM D746
LyondellBasell Alathon® 9301 High Density Polyethylene
ApplicationsALATHON 9301is a high density resin designed for sheet extrusion and thermoforming. It exhibits very low sag and high stiffness.Regulatory StatusALATHON 9301 meets the requirements of F..
Copyright © lookpolymers.com All Rights Reserved