Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=3.00 mm |
167 °F @Thickness >=0.118 in |
|
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=2.50 mm |
167 °F @Thickness >=0.0984 in |
|
LG Chemical AF312T ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=0.800 mm |
167 °F @Thickness >=0.0315 in |
|
LG Chemical Lupox® GP2400G PBT+GF40% Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=0.800 mm |
167 °F @Thickness >=0.0315 in |
|
LG Chemical Lupox® NH2306F PBT+GF30% Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=0.500 mm |
167 °F @Thickness >=0.0197 in |
|
LG Chemical Lupox® TE5006F PET+PC Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0590 in |
UL 746 |
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0590 in |
UL 746 |
Teknor Apex Chemlon® 212 Nylon 6, Unreinforced Features: Lubricated, General Purpose; General purpose nylon 6; Slightly tougher and more ductile than nylon 66 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.930 mm |
167 °F @Thickness 0.0366 in |
UL746B |
DSM Arnite® A06 101 PET (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.60 mm |
167 °F @Thickness 0.0630 in |
|
Eurostar Starflam R10002E PA66/6, Injection Molded Starflam R10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 66/Polyamide 6 Injection Molding Resin (also known as R1000Z220EM)Information provided by Polymer Te.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.750 mm |
167 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.750 mm |
167 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.810 mm |
167 °F @Thickness 0.0319 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL746B |
DSM Arnite® T06 204 SN PBT (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |