| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Bead Filled |
| Manufacturer | Polyram |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polyram RamSter PF340S4 PBT, 20% Glass Beads.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
| Water Absorption at Saturation | 0.5 % | 0.5 % | ISO 62 |
| Linear Mold Shrinkage | 0.02 cm/cm | 0.02 in/in | ISO 2577 |
| Melt Flow | 15 g/10 min <br>@Load 2.16 kg,<br> Temperature 250 °C |
15 g/10 min <br>@Load 4.76 lb,<br> Temperature 482 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 50.0 MPa | 7250 psi | ASTM-D638 |
| Elongation at Break | 5 % | 5 % | ASTM-D638 |
| Tensile Modulus | 3.20 GPa | 464 ksi | ASTM D638 |
| Flexural Strength | 80.0 MPa | 11600 psi | ASTM D790 |
| Flexural Modulus | 2.10 GPa | 305 ksi | ASTM-D790 |
| Izod Impact, Notched | 0.350 J/cm <br>@Temperature 23.0 °C |
0.656 ft-lb/in <br>@Temperature 73.4 °F |
ASTM-D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 225 °C | 437 °F | ISO 11375 |
| Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75 |
| Flammability, UL94 | HB <br>@Thickness 3.00 mm |
HB <br>@Thickness 0.118 in |
IEC 60695 |
| Glow Wire Test | 650 °C | 1200 °F | GWFI |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1e+15 ohm | 1e+15 ohm | IEC 60093 |
| Dielectric Constant | 3.6 <br>@Frequency 1e+6 Hz |
3.6 <br>@Frequency 1e+6 Hz |
IEC 60250 |
| Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60250 |