Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® 123HSR PC (Asia Pacific) Easy flow, UV stabilised, super release grade polycarbonate. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® 241RX PC (Europe-Africa-Middle East) LEXAN 241RX is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.75 mm and allows for the molder to use up to 50 percent regri.. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® 4501 PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® BY2710X PC (Asia Pacific) BY2710X is a modified Polycarbonate (PC) resin. It is a non-filled, injection moldable grade with UL-94 V0 rating and is available in various opaque color options. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | |
PTS Tristar® PC-10FR-(VIK) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Impact Modifier and Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | |
PTS Tristar® PC-10R-(18) 18 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | |
PTS Tristar® PC-10R-(22) 22 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | |
PTS Tristar® PC-10R-(V15) 15 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | |
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | |
PTS Tristar® PC-10R-CL(V15) 15 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® HF1110R PC (Europe-Africa-Middle East) LEXAN HF1110R is a high flow grade especially designed for applications that require thin wall sections and high flow lengths. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX2010T_ PC (Europe-Africa-Middle East) Global grade. LEXAN LUX2010T is an injection moulding grade especially designed for manufacturing optical parts requiring excellent flow properties combined with very high transmission and color sta.. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX2910T_ PC (Europe-Africa-Middle East) Global grade. LEXAN LUX2910T is an injection moulding grade especially designed for manufacturing optical parts requiring superior flow properties combined with very high transmission and color stab.. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® 4501 PPC High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® 945 PC (Europe-Africa-Middle East) Lexan* 945 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | |
PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | |
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | |
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | |
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm.. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Valox® 553U PBT+PC 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.47 mm |
257 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® LV-2225L Standard (mold release/ice color grade) Polycarbonate Resin Flame retardant and mold release grade with high fluidity, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for thin wall injection moldings.Applications:Electric, ele.. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746 |
Styron EMERGEâ„¢ 4630-10 Polycarbonate EMERGEâ„¢ PC 4630-10 advanced resin is formulated to supply both excellent ultraviolet stability and enhanced ignition resistance while maintaining excellent physical properties and processabilit.. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746 |
Styron EMERGEâ„¢ 4850-10 Polycarbonate EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746 |
Styron EMERGEâ„¢ 8600-10 Polycarbonate EMERGEâ„¢ PC 8600-10 is a translucent, ignition-resistant polycarbonate resin. The resin contains no bromine, chlorine or phosphate additives and is intended to comply with global environmental .. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Europe-Africa-Middle East) |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East) VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |