Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Asia Pacific) CYCOLOY C6600 is a FR PC+ABS of nonbrominated, nonchlorinated flame retardant systems with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipm.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY5210 PC+ABS (Europe-Africa-Middle East) CYCOLOY CY5210 is a flame retardant PC/ABS using non-chlorinated and non-brominated FR additives for injection moulding. CYCOLOY CY5210 has an improved hydrolytic stability with balanced flow and im.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® BFL2010 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® BFL2010 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® EM3110 PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL403 PC Various weight reductions at 0.250"" wall. UV-resistant. Impact resistant, Superior processing, excellent surface. UL94 V-0/5V at 0.125"". |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL900S PC (Europe-Africa-Middle East) Foamable Lexan* FL900S polycarbonate resin is an ideal choice for structural components where load bearing capability at elevated temperature is a key requirement. It exhibits outstanding inpact str.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD4211 PC (Europe-Africa-Middle East) Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD4472 PC (Europe-Africa-Middle East) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML3041 PC (Europe-Africa-Middle East) LEXAN ML3041 has been developed for the injection moulding of thin-wall, complex parts that require high mechanical properties and impact resistance.This data was supplied by SABIC-IP for the Europe.. |
|||
UL RTI, Mechanical without Impact | 80.0 - 130 °C | 176 - 266 °F | Average value: 107 °C Grade Count:13 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.750 - 0.800 mm |
176 °F @Thickness 0.0295 - 0.0315 in |
|
LG Chemical LUPOY GP2102 PC+GF10% Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.60 - 1.70 mm |
176 °F @Thickness 0.0630 - 0.0669 in |
|
LG Chemical LUPOY RF3208F PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2 and 13463-67-1Information provided by LG .. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | |
LG Chemical LUPOY SR3108L PC, High Impact Description: Injection Molding, PC, High Flow, High Impact, White Color OnlyApplication: BLU Mold frame for Mobile DevicesCAS: 103598-77-2 and 13463-67-1Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.500 - 2.50 mm |
176 °F @Thickness 0.0197 - 0.0984 in |
|
LG Chemical Lupoy 3010-30 Polycarbonate Resin Description: LUPOY PC 3010-30 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC LNP* Lubricomp* Lexan_LF1510A compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Asia Pacific) 10% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1520 compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1530A PC LNP* Lubricomp* Lexan_LF1530A compound is a 30% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON DX89795 PC (Europe-Africa-Middle East) LNP* STATKON* DX89795 is a compound based on Polycarbone resin containing Carbon Powder. Added features include: Electrically Conductive, Easy Molding, Mold Release. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL746-B |
Shuman 791 Black and Custom Colors ABS-Flame Retardant Long term thermal aging rated. Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
Covestro Makrolon® FR 7067 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
Covestro Makrolon® FR 7087 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
Diamond Polymers ABS 2512 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
Diamond Polymers ABS 3502ELG Description: Injection Molding Grade, Medium Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.47 mm |
176 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® BN-8120R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD4413 PC (Europe-Africa-Middle East) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML3485 PC (Europe-Africa-Middle East) LEXAN ML3485 is a low viscosity grade exhibiting an improved ductility over standard polycarbonate grades at equal flow. |