Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | 120°C/h; ISO 75/1 |
Polykemi AB SCANMID 6 B12^ F20 NH6 Nylon 6, Glass Fiber Reinforced, Halogen Free, Flame Retardant Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ASTM D648 |
Polymer Resources TP-GFMF2 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced Polybutylene Terephthalate, 40% Glass/Mineral ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ISO 75-1,-2 |
Lanxess Durethan® BKV 135 DUS008 000000 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | |
LATI Larton MDT16-02 PPS Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & M.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | |
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongationAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Amer.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | V-notch; ISO R 75 |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2 Filled, Heat Stabilized, Dry Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C @Thickness 6.40 mm |
410 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM 2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C @Thickness 6.40 mm |
410 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C @Thickness 3.20 mm |
410 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C @Thickness 3.20 mm |
410 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C @Thickness 6.40 mm |
410 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics ULTEM 1000EF PEI Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP 9X11428J PPS LNP* THERMOCOMP* 9X11428J is a compound based on Polyphenylsulfone containing Proprietary Fillers. Added features of this material include: Healthcare, Low Extractable. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® N110L (Dry) Nylon 6, 10% Glass Fiber Reinforced, Lubricated Features: LubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600 MR 309 HWCP 30% Mineral Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | 1/4''; ASTM D648 |
Ensinger TECAPEI® made from Ultem® 1000 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ISO 75 |
Eurotec® Tecodur® PB70 GR15 BK002 WX21 PBT, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ISO 75-1/2 |
Eurotec® Tecomid® NA40 MR30 NL PA 6.6 30% mineral reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ASTM D648 |
Adell BR-13 Nylon 6, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ISO 75 |
BASF Ultramid® B3WGM24 HPX BK 2320 30% Glass/Mineral Filled PA6 (Dry) Description: Ultramid B3WGM24 HPX BK23210 is a very high productivity, 30% glass/mineral reinforced heat stabilized injection molding PA6 grade for components that require medium rigidity, excellent.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ASTM D648 |
Ashley Polymers Ashlene® P123WO PBT Polyester, 15% Glass Reinforced PBT polyester with 15% glass reinforcement, flame retardant.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ASTM D648 |
BLUESTAR 201G25 PBT, 25% Glass Filled Typical Applications: Energy saving lightingInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ISO data |
BASF Capron® 8331G HS Blend Impact Modified, 14% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8331G HS Blend is a 14% glass fiber reinforced, heat stabilized, polyamide 6 molding compound developed for applications requiring improved toughness in combination with a balance of strength.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ISO 75 |
BASF Ultradur S 4090 G4 High Speed Unc. 20% Glass Filled PBT Ultradur S 4090 G4 High Speed Unc. is a high flow, fast cycling with low warpage, 20% glass filled injection molding PBT for industrial parts, rigid tough and dimensional stable applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | |
Radici Radiflam® A AE (dry) Nylon 66 Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |