| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled |
| Manufacturer | Adell Plastics, Inc. |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Adell BR-13 Nylon 6, 15% Glass Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
| Water Absorption | 1.5 % | 1.5 % | 24 hour immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 88 | 88 | ASTM D785 |
| Hardness, Rockwell R | 119 | 119 | ASTM D785 |
| Tensile Strength, Ultimate | 100 MPa | 14500 psi | ASTM D638 |
| Elongation at Break | 4.5 % | 4.5 % | ASTM D638 |
| Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
| Flexural Modulus | 5.00 GPa | 725 ksi | ASTM D790 |
| Compressive Yield Strength | 103 MPa | 14900 psi | ASTM D695 |
| Izod Impact, Notched | 0.500 J/cm | 0.937 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 222 °C | 432 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 193 °C | 379 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |