Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
ASTM D648
Shell Carilon® D26VM100 Polyketone, High-Flow Injection Molding Grade  (discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26VM100 is a high-flow injection molding grade with mechanical properties which classify it as an ..
Deflection Temperature at 0.46 MPa (66 psi) 203 °C

@Thickness 3.20 mm
397 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI
LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP Lubricomp EL004 PEI
LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas..
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific)
LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac..
Deflection Temperature at 0.46 MPa (66 psi) 203 °C

@Thickness 3.20 mm
397 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA 6/10 (Asia Pacific)
LNP* Lubricomp* QAP22S is a compound based on Nylon 6/10 resin containing PTFE, Aramid Fiber, Silicone. Added features of this material include: Internally Lubricated, Heat Stabilized.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C

@Thickness 3.20 mm
397 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA6.10
LNP* LUBRICOMP* QAP22S is a compound based on Nylon 6/10 resin containing 10% PTFE/Silicone, 10% Aramid Fiber. Added features of this material include: Wear Resistant, Heat Stabilized.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66
LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP RFL46 PA6.6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RFL46 is a compound based on PA66 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP STAT-KON EX11402 PEI
LNP* STAT-KON* EX11402 is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT
LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C

@Thickness 3.20 mm
397 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI
LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C

@Thickness 3.20 mm
397 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific)
LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12
LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C

@Thickness 3.20 mm
397 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12
LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 (Asia Pacific)
LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C

@Thickness 3.20 mm
397 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 (Asia Pacific)
LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP Thermocomp PFB139E PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PFB139E is a compound based on PA 6 resin containing Glass Fiber, Glass Bead, Flame Retardant. Added features include; Flame Retardant, Easy Molding.This data was supplied by SABIC-..
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Bf
Eurostar Starflam PFB139E PA6, Glass Fiber/Bead Filled, Flame Retardant, Injection Molded
Starflam PFB139E is a Flame Retardant Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding Resin (also known as PFB1013Z590)Information provided by Eurostar.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
ASTM D648
Ashley Polymers Ashlene® 528MS/528SMS Nylon 66, MoS2 Filled
A general purpose Molybdenum-disulfide filled nylon resin.Data provided by the manufacturer
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
ASTM D648
Beijing Ranger Chem PBT-201-G10 272 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
ASTM D648
A. Schulman ComAlloy Hiloy® 616 Nylon 6, Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Deflection Temperature at 0.46 MPa (66 psi) 203 °C
397 °F
ASTM D648
Ashley Polymers Ashlene® 520 Nylon 66
A general purpose basic Nylon 66 resin, slightly lubricated.Data provided by the manufacturer