Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | Unannealed; ASTM D648 |
Multibase Nylex™ 4032 Black Polyamide + PP Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Network Polymers Kepital® F10-02 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Network Polymers Kepital® F20-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
PTS POM-90 9.0 MFI Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPH GF10030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Kolon KOCETAL® K200 Standard Grade Acetal Resin Suitable for both injection and extrusion.Applications: Injection and extruded use such as rod and sheetInformation provided by API Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Kolon KOCETAL® K500 Standard Grade Acetal Resin General injection molding grade. Easy flow grade for hard-to fill molds and mechanical thin-wall parts.Applications: General injection molding products.Information provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Kolon KOCETAL® LW701 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | |
Aardvark Polymers AARTEL® 820UV Acetal Copolymer Rotational Molding Resin Aartel 820UV is a natural acetal copolymer with added UV stabilizers.Aartel 820UV is a low viscosity resin with excellent flow characteristics.Aartel 820UV is available in natural white and may be p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
KEP Kepital® F30 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
IRPC Polimaxx Polene 2311LCX GA4 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 20% GLASS FIBRE REINFORCED, HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, HIGH STIFFNESS, LOW SHRINKAGEAPPLICATIONS: INJECTION MOLDING FOR AUTOP.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ISO 75-1/-2 |
Lanxess Durethan® DP BC 310 EF 600065 Nylon 6 PA 6, injection molding and extrusion grade, non-reinforced, elastomer modified, high impact strength, good flowability (Easy Flow) |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C @Thickness 3.20 mm |
316 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C @Thickness 3.20 mm |
316 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY K2000XXH Acetal LNP LUBRILOY* K2000XXH is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material are: Wear Resistant, Healthcare. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C @Thickness 3.20 mm |
316 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Asia Pacific) 40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100TL NC010 (formerly Delrin 100TL NC000) is a high viscosity acetal homopolymer with 1.5% TeflonInformatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
E-Polymers TEKAPPO® J930 30% Glass Fiber Reinforced M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Ensinger Tecaform™ FG Blue Food Grade Acetal (POM) Tecaform™ is resistant to hot water and typical cleaning chemicals. It possesses good bearing and wear properties. The blue color makes it more visible than standard grades. It is commonly used .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin 100TL is a high viscosity acetal homopolymer containing 1.5% Teflo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Aclo Accucomp Polyacetal (POM) ACE091L High Viscosity |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | |
BASF Procom® GC20S 400 Polypropylene Uses: electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Ashley Polymers Ashlene® 190 Acetal A general purpose, medium viscosity, natural.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Ashley Polymers Ashlene® 197-N2 Acetal A general purpose, very low viscosity, in natural.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Asahi Kasei Tenac®-C EX351 Acetal Copolymer, Extrusion Grade
(discontinued **) High-viscosity grade amenable to extrusion.Applications: Extruded rods and sheets.This product is not a part of the standard product line dated 2003. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
Mitsubishi Iupital® F10-02 High Viscosity Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
RheTech Products GC20P100-01 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 158 °C | 316 °F | ASTM D648 |
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products. |