Material Notes:
Tecaform™ is resistant to hot water and typical cleaning chemicals. It possesses good bearing and wear properties. The blue color makes it more visible than standard grades. It is commonly used as bushings, rollers, wear strips and other applications requiring a combination of strength, low moisture absorption, chemical resistance, and dimensional stability.Features:No centerline porosityLow moisture absorptionexcellent machinabilityGood combination of mechanical propertiesResistance to food industry cleaning chemicals, including aqueous solutions with pH between 4 and 14Good wear and abrasion propertiesManufactured from resin and color components that are FDA, USDA, and 3A Dairy compliantGood dimensional stabilityGood property retention at elevated temperaturesInformation supplied by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 0.22 %
0.22 %
24 hrs; ASTM D570
Water Absorption at Saturation 0.80 %
0.80 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 86
86
ASTM D785
Tensile Strength, Yield 60.7 MPa
8800 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 2.62 GPa
380 ksi
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Compressive Strength 31.0 MPa
4500 psi
ASTM D695
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.21
0.21
40 psi, 50 fpm; ASTM D3702
K (wear) Factor 131 x 10-8 mm³/N-M
65.0 x 10-10 in³-min/ft-lb-hr
vs steel; 40 psi, 50 fpm; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 84.6 µm/m-°C
47.0 µin/in-°F
ASTM D696
Melting Point 165 °C
329 °F
ASTM D2133
Maximum Service Temperature, Air 90.6 °C
195 °F
Long Term; UL 746B
141 °C
285 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
316 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.0e+14 ohm-cm
1.0e+14 ohm-cm
ASTM D257
Dielectric Constant 3.7

@Frequency 60 Hz
3.7

@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 19.7 kV/mm
500 kV/in
ASTM D149
Dissipation Factor 0.001

@Frequency 60 Hz
0.001

@Frequency 60 Hz
ASTM D150