Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648-95 |
Multibase Multi-Pro® 2518 CU 25% Mineral Filled Polypropylene Multi-Pro 2518 CU is a mineral reinforced polypropylene compound offering overall balanced impact and stiffness properties. This material is specially formulated with UV stabilization for outdoor ex.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 3.18 mm |
216 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Maxxam™ DP 9052-3-1000 Polyethylene, High Density (HDPE) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | Method A, flatwise, unannealed; ISO 75-1/2 |
Mytex Polymers AS319LW-01US Thermoplastic Polyolefin, 19% Talc Filled AS319LW-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural, g.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | |
Eastman Eastalloy DA105 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ISO 75 |
Phillips Sumika Marlex® CHP-370 Thermoplastic Polyolefin
(discontinued **) Thermoplastic Polyolefin, Good Stiffness and Impact PerformanceApplications: Automotive Pillar TrimConditioning after Molding: 48 hr at 23°CNominal Shrinkage: 0.8-1.0%Drying conditionsTemperature: .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | Unannealed; ASTM D648 |
PolyOne Edgetek® AS-30GF/000 BLACK Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
Flint Hills AP5135-HS Impact Copolymer Polypropylene Medium impact copolymer, FDA compliantFeatures: Nucleated and heat stabilized.Applications: Injection molding: large, thin wall automotive interior parts and housewares.Former Huntsman polypropylene.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ISO 75B |
Lucite International Diakon® MG100 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 6.40 mm |
216 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL SE100X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/V1 rated. RTI Elec/Imp/Str 95/80/95. Good flow. Suitable for E/E market indoor/outdoor applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 6.40 mm |
216 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL SE100X PPE+PS (Asia Pacific) Nonbrominated, nonchlorinated FR resin. Improved productivity and reliability. 199F HDT. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Asia Pacific) PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP AFB42 ABS LNP* THERMOCOMP* AFB42 is a compound based on ABS containing 10% Glass Fiber, 20% Glass Bead. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ISO 75-1/-2 |
Styrolution Luran® 388 S SAN Description: Specialty grade with highest mechanical strength and chemical resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | annealed; ASTM Test |
Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 3.17 mm |
216 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 3.17 mm |
216 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
A. Schulman PP 1667-01 Polypropylene Natural Homopolymer Polypropylene DescriptionPolypropylene PP 1667-01 is an easy flowing natural homopolymer polypropylene. It is for injection molding large parts with thin sections requiring good stiffness, heat resistance, and c.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 3.17 mm |
216 °F @Thickness 0.125 in |
ISO 75 |
A. Schulman FORMION™ FI 232 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232 is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.App.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 100ST BK602 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST BK602 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | 0.125";; ASTM D648 |
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
Aclo Accutech ABS ABS833G40L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
Ineos H14A-00 Polypropylene Homopolymer Suggested fabrication methods: Injection molding and extrusion applications.Features: AntistaticTypical applications: Packaging, Closures, Consumer productsComplies with FDA specification, Title 21,.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
Buckeye Polymers BP RPP 1010 T Polypropylene, 10% Mineral Filled This Talc-filled product exhibits excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resis.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY XP4025 ASA+PC Available in a wide range of colors and is recommended for unpainted exterior applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
Samyang Triel® 5550 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5550 is an extrusion grade.Information provided by Samyang. |