Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C @Thickness 3.20 mm |
181 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® FR23 ABS Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C @Thickness 3.20 mm |
181 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® FR23 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers MS 160 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Network Polymers NPP 20-2501 C/AS Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs V0E ABS, Flame Retardant Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ISO 75/Method Bf |
Premix Thermoplastics PRE-ELEC® PS 1328 PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | |
Polycasa Acryl® KR 2015/1 Acrylic, Impact Grade Medium-impact grade with very good flow behavior, especially mechanically stressed parts with long flow paths; e.g. strip light diffusers. Can be extruded into thin tubes, sheet and film.Data was c.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
SABIC PP 674K Polypropylene Copolymer for Injection Molding Product Description: PP 674K is specially developed for producing injection molded & ISBM articles with high clarity and also has better impact properties than homo PP counterparts.PP 674K has the .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.8 - 100 °C | 181 - 212 °F | Average value: 94.2 °C Grade Count:37 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.8 °C | 181 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 - 210 °C | 181 - 410 °F | Average value: 160 °C Grade Count:22 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | |
LyondellBasell Lupolen® 5621 D HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Flint Hills P5L2Z-038 Random Copolymer Polypropylene Random copolymer, USP Class VI certified, and FDA compliant.Features: Hydrotalcite.Applications: Injection molding: extrusion blow molding and hot fill applications.Former Huntsman polypropylene pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C @Thickness 6.40 mm |
181 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ISO 75 |
LyondellBasell Hifaxâ„¢ CB228 Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good paintability, good processabilityApplications: aut.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C @Thickness 6.40 mm |
181 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY 63000CT PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C @Thickness 6.40 mm |
181 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTU PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency, UV cut, and superior cleanliness for advanced semiconductor packaging applications |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | Annealed; ISO 75-2A |
Total PSC 1540(EU) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite 105E3V36327 Acetate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite 360E461312 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite Propionate 383A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | |
BASF Polystyrol® 475 K Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade with particularly good creep strength.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Braskem CP 141 Injection Molding Polypropylene Description: CP 141 is a high melt flow rate heterophasic copolymer specially designed to achieve high productivity on thin-walled parts with very easy mould filling and high speed injection mouldin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Braskem CP 144 Coating Polypropylene Information provided by Braskem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.8 °C | 181 °F | ASTM D648 |
Americas Styrenics MC3700 High Heat Crystal Polystyrene Product CharacteristicsEasy filling of thin-walled partsExceptional mold releaseImproved cycle times in hard to fill partsFood Contact CompliantUL Classification 94HBUSP Class VITypical Applications.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612
(Unverified Data**) Zytel® LC6210 BK010 is a highly toughened, heat stabilized polyamide 612 for extrusion, blow molding or processing by other techniques requiring high melt viscosity. It was previously coded Zytel®.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ISO 75-2 |
Borealis Daplen™ EF103AE Polypropylene TPO Compound Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite Butyrate 465A3720010 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 10%. Weight loss on heating = 0.9% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |