Material Notes:
Information provided by Braskem
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792A
Melt Flow 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 77
77
ASTM D785
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.12 GPa
162 ksi
ASTM D790
Izod Impact, Notched 0.340 J/cm

@Temperature -20.0 °C
0.637 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
0.700 J/cm

@Temperature 23.0 °C
1.31 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
ASTM D648
Vicat Softening Point 147 °C
297 °F
-1kg; ASTM D1525