Material Notes:
Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
2 in per min; ASTM D638
Elongation at Yield 10 %
10 %
chs 2 in/min; ASTM D638
Flexural Modulus 0.827 GPa
120 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
ASTM D648