Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C @Thickness 3.20 mm |
181 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® FR23 ABS Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers MS 150 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Network Polymers MS 160 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs V0E ABS, Flame Retardant Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYelast TPE EC12 D55 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | 75/Method Bf |
Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ISO 75/Method Bf |
Premix Thermoplastics PRE-ELEC® PS 1328 PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | Unannealed; ASTM D648 |
Phillips 66 COPYLENE® CM003 Polypropylene Impact Copolymer CM003 is a fractional melt flow impact copolymer with a barefoot additive package which is specially formulated to excel in extrusion processes.Applications: Extrusion ProcessesInformation provided .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
SABIC PP681K Polypropylene Random Copolymer for Injection Molding Product Description: PP 681K is specially developed for producing injection molded articles with high clarity and also has better impact properties than homo PP counterparts.PP 681K has the followi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 - 210 °C | 181 - 410 °F | Average value: 160 °C Grade Count:22 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Flint Hills P5L2Z-038 Random Copolymer Polypropylene Random copolymer, USP Class VI certified, and FDA compliant.Features: Hydrotalcite.Applications: Injection molding: extrusion blow molding and hot fill applications.Former Huntsman polypropylene pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C @Thickness 6.40 mm |
181 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C @Thickness 6.40 mm |
181 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY 63000CT PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C @Thickness 6.40 mm |
181 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTU PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency, UV cut, and superior cleanliness for advanced semiconductor packaging applications |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ISO 75-1/-2 |
Styrolution Polystyrol 486 M GR 2 PS Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Borealis Bormed™ RB845MO Random Copolymer for Healthcare Applications Bormed RB845MO is a random copolymer for blow molding with very good transparency and high contact clarity, very good gloss and surface finish. Bottles in sizes up to 2 quarts molded from Bormed RB.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
TPI Porene® ABS-AN450 Flame Retardant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite Propionate 376E4000012 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite Propionate 377E4861312 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Eastman Tenite Propionate 383A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM-D648 |
Braskem PRB 0131 RACO Random Polypropylene Copolymer PRB 0131 is a low melt flow rate random copolymer with high transparency. This resin is designed for thermoforming, blow molding, and extrusion. This product exhibits excellent processability, low h.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | |
BASF Polystyrol® 475 K Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade with particularly good creep strength.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | |
BASF Polystyrol® 476 L Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade. When extruded it is often mixed with PS 165 H.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | |
BASF Polystyrol® 486 M Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H). Suitable for dairy packaging.Data was co.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Braskem CP 141 Injection Molding Polypropylene Description: CP 141 is a high melt flow rate heterophasic copolymer specially designed to achieve high productivity on thin-walled parts with very easy mould filling and high speed injection mouldin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
Braskem CP 144 Coating Polypropylene Information provided by Braskem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 83.0 °C | 181 °F | ASTM D648 |
LyondellBasell Astryn 73A6-3 Polypropylene Copolymer, 30% Calcium Carbonate Key Features: medium high melt flow, medium modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, excellent chemical resistance, excellent aesthetics, high gloss, .. |