Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem PRB 0131 RACO Random Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Braskem PRB 0131 RACO Random Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PRB 0131 is a low melt flow rate random copolymer with high transparency. This resin is designed for thermoforming, blow molding, and extrusion. This product exhibits excellent processability, low haze, and excellent impact strength. Its applications include: high transparency thermoformed packaging for food, cosmetics, hygiene, and cleaning products; bottles for food, cosmetics, and cleaning products; returnable water bottles; and high transparency sheets, toy kits, and cosmetic packages.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM-D792
Melt Flow 1.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79
79
ASTM-D785
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM-D638
Elongation at Yield 13 %
13 %
ASTM-D638
Flexural Modulus, 1% Secant 900 MPa
131000 psi
ASTM-D790
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °C
181 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C
118 °F
ASTM-D648
Vicat Softening Point 130 °C

@Load 1.02 kg
266 °F

@Load 2.25 lb
ASTM-D1525
Optical Properties Metric English Comments
Haze 24 %

@Thickness 1.00 mm
24 %

@Thickness 0.0394 in
ASTM-D1003