Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ISO 75 |
Nilit FRIANYL B63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ISO 75 |
Nilit FRIANYL B63 CV20 Nylon 6.6 for injection molding, 20% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | |
Radici Radilon® A ERV3012 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | |
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified. Used in Automotive Electronics applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C @Thickness 6.40 mm |
464 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa PET-RG30 Flame Retardant, 30% Glass Fiber Reinforced PET Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C @Thickness 6.40 mm |
464 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ASTM D648 |
Fiberfil® M-2501 BK Nylon 66, 40% mineral Filled, post industrial Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP RF003ES PA 66 LNP* THERMOCOMP* RF003ES is a Nylon 66 base resin containing 15% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C @Thickness 3.20 mm |
464 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE) LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL GTX GTX230 PPE+PA66 (Europe-Africa-Middle East) |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | DIN 53461 |
Polyram PlusTek PA870G33 Nylon 6.6, 33% Glass Fiber 33% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ASTM D648 |
Toyobo Vylopet® EMC317R Glass Reinforced Polyester, Standard Grade Key Feature: UL-94 classApplications: Glossy surface componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, ch.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ASTM-D648 |
Toyobo VYLOPET® EMC320R Polyester Resin VYLOPET® is a polyester resin developed specifically for injection molding. Polyester resins have excellent heat resistance, rigidity, chemical resistance, and electric properties. Grade EMC320R ha.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 240 °C | >= 464 °F | DIN 53461 |
Polyram PlusTek RA300G4 Nylon 6.6, 20% Glass Fiber 20% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ASTM D648 |
Toyobo VYLOPET® EMC532 Injection Molding Polyester Resin, Glass Reinforced Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ASTM D648 |
Cheng Yu Plastic N6CV3 Flame Retardant Nylon 6, 30% Mineral Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | dry; ISO 75-1/-2 |
DSM EcoPaXX® Q-PG6 PA410-I-GF30 % Glass Reinforced, Impact Modified |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600/50 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600/58 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ASTM D648 |
Clariant Renol PA113G15 Nylon 66, 15% Glass Fiber Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ASTM D648 |
Clariant Renol PA143G10 Nylon 6/66 Copolymer, 10% Glass Fiber, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ISO 75 |
Eurotec® Tecopet® PT70 GR30 NL100 HT PET, 30% glass fiber reinforced, high heat stabilized, natural Information provided by Eurotec® |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ASTM D648 |
E-Polymers TEKAMID® TA250G15 , 15% Glass Fiber Reinforced PA66, DAM 15% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ISO 75 |
BASF Petra® 130 30% Glass Filled PET Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ISO 75 |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ISO 75 |
BASF Petra® 130 FR 30% Glass Filled PET Petra 130 FR is a 30% glass fiber reinforced, flame retardant injection molding polyethylene terephthalate feedstocks. It is recognized as UL 94V-0/5VA by Underwriters Laboratories. It is also avail.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ISO 75 |
BASF Petra® 130 FR BK-112 30% Glass Filled PET Petra 130 FR BK-112 is a 30% glass fiber reinforced, black pigmented, flame retardant injection molding compound based on post-consumer and post-industrial recycle polyethylene erephthalate feedstoc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | ISO 75 |
Polyram PlusTek RA325G4 Nylon 66 for Injection Molding, 20% Glass-Fiber Reinforced, Self-Extinguishing, Halogen Free 20% Glass-fiber reinforced, self-extinguishing halogen free Nylon 66 for injection molding applications.Information provided by Polyram. |