Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75 |
Nilit FRIANYL A63 EO Raw extruded nylon 6.6 for injection molding Raw extruded nylon 6.6 for injection molding, with surface lubrication.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Unannealed; ISO 75-2/B |
PolyOne Bergamid™ A700 TM-YF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75 |
Nilit FRIANYL B63 W-KV20 Nylon 6 for injection molding, 20% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DIN 53461 |
Qualchem Danamid FGFS-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Impact modified.Information provided by Qualchem Zrt. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ASTM D648 |
LG Chemical Lupox® PBT-LW5303 30% Glass Filled Low Warp PBT Low Warpage. Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 - 210 °C | 392 - 410 °F | ASTM D1525, HDT Method B |
Loxim 210 01HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN173MC M/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics ULTEM 1010R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics ULTEM 1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). UL94 V0, V2 and 5VA listing. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics ULTEM HU1010 PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics ULTEM MD141 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C @Thickness 3.20 mm |
392 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON ZX08301 PPE (Asia Pacific) Stat-Kon* ZX08301 compound is a high heat compounds with ESD safe and low warpage performance suitable for use in Semiconductor Packaging Applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C @Thickness 3.20 mm |
392 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | 0.25 inch; ASTM D648 |
PlastxWorld CEVIAN® B5524 20% GF PBT/ABS Alloy Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DIN 53461 |
Polyram PlusTek PA340S6 Nylon 6.6, 30% Glass beads 30% glass beads reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ASTM D648 |
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66 Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 200 °C | >= 392 °F | DIN 53461 |
Polyram PlusTek RA300G3 Nylon 6.6, 15% Glass Fiber 15% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ASTM D648 |
Beijing Ranger Chem PBT-201-G15 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75-1/-2 |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 101L BKB009 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L BKB009 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75-1/2 |
Eurotec® Tecomid® NB40 KK30 NL IL PA 6 30% glass fiber/mineral reinforced, impact modified, low warpage Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75 |
Eurotec® Tecomid® NB400 GR15 NL MB PA6, 15% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ASTM D648 |
Ashley Polymers Ashlene® 524 Nylon 66 A general purpose toughened Nylon 66.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics ULTEM 1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be sup.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics ULTEM 1000EF PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS. US FDA and EU Food Contact compliant. |