Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | RT |
Outokumpu 4565 High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | RT |
Outokumpu 4742 High Temperature Ferritic Stainless Steel Good scaling resistance and can be subjected to reducing sulphur environments without risk. Subject to 475°C embrittlement and grain coarsening at temperatures above 950°C. s-phase may form afte.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Plansee Chromium, Cr; Sintered Characteristics:High corrosion resistanceHigh wear resistanceBeautiful opticsLower melting point than other refractory metalsVery high vapor pressureLower density than other refractory metalsPossess.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 20.0 °C |
0.108 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel URANUS® B28 High Nickel Super-Austenitic Stainless Steel Description: URANUS® B28 (UR B28) is a super-austenitic stainless steel with very high nickel (31%) and chromium (27%) contents. The molybdenum content is about 3.5%. The alloy is designed for sp.. |
|||
Specific Heat Capacity | 0.452 J/g-°C | 0.108 BTU/lb-°F | RT |
Haynes 214® alloy sheet Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.452 J/g-°C | 0.108 BTU/lb-°F | RT |
Haynes 214® alloy, 20% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.452 J/g-°C | 0.108 BTU/lb-°F | RT |
Haynes 214® alloy, 50% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.452 J/g-°C | 0.108 BTU/lb-°F | RT |
Haynes 214® alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.452 J/g-°C | 0.108 BTU/lb-°F | RT |
Haynes 214® alloy, sheet, 100 hours exposure at 870°C (1600°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.452 J/g-°C | 0.108 BTU/lb-°F | RT |
Haynes 214® alloy, sheet, 100 hours exposure at 980°C (1800°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.452 J/g-°C | 0.108 BTU/lb-°F | RT |
Haynes 214® alloy, sheet, 1000 hours exposure at 870°C (1600°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.452 J/g-°C | 0.108 BTU/lb-°F | RT |
Haynes 214® alloy, sheet, 32 hours exposure at 760°C (1400°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.452 J/g-°C | 0.108 BTU/lb-°F | RT |
Haynes 214® alloy, 10% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.452 J/g-°C | 0.108 BTU/lb-°F | RT |
Haynes 214® alloy, 30% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 500 °C |
0.108 BTU/lb-°F @Temperature 932 °F |
|
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 500 °C |
0.108 BTU/lb-°F @Temperature 932 °F |
|
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 500 °C |
0.108 BTU/lb-°F @Temperature 932 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Special Metals BRIGHTRAY® Alloy F Electrical Resistance Alloy A nickel-iron-chromium electrical-resistance alloy for use at temperatures up to 1920°F (1050°C) under continuous operating conditions. Its high iron content and relatively low level of nicke.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.5 x 2.0 inch (13 x 51 mm) Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 0.5 x 2.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.62 inch (16 mm) Diameter Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 0.62 in.. |
|||
Specific Heat Capacity | 0.452 J/g-°C | 0.108 BTU/lb-°F | |
Special Metals INCONEL® Alloy G-3 A nickel-chromium-iron alloy with additions of molybdenum and copper. It has good weldability and resistance to intergranular corrosion in the welded condition. The low carbon content helps preven.. |
|||
Specific Heat Capacity | 0.453 J/g-°C | 0.108 BTU/lb-°F | |
Special Metals INCONEL® G-3 Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
ThyssenKrupp XABO® 500 Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Carpenter 20-Mo6® Stainless Steel, Plate Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
ATI Allegheny Ludlum Type 317 Stainless Steel, UNS S31700 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 21.0 °C |
0.108 BTU/lb-°F @Temperature 69.8 °F |
|
Haynes R-41 alloy, Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications include .. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
ThyssenKrupp XABO® 460 T Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |