Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® DMX2415 PC Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Americ.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East) Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 80.0 °C |
0.335 BTU/lb-°F @Temperature 176 °F |
DSC |
Eastman Heatwave CF746 Polymer
(discontinued **) Heatwave is a clear, reheat enhanced, PET polyester designed for heatset containers containing a UV light protection package chemically bound to the backbone of the polymer. Pellets are 2.5 mm (0.1 .. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 80.0 °C |
0.335 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman Vitiva PC715 PET
(discontinued **) Vitiva PET PC715 is an exceptionally clear PET polyester that contains a UV light protection package chemically bound to the backbone of the polymer. This non-extractable UV inhibitor absorbs damagi.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman Aqua 18696 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 80.0 °C |
0.335 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman Aqua 20837 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer 20.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman 9663 PET
(discontinued **) VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 80.0 °C |
0.335 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman 9921P PET Film
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | Average value: 1.40 J/g-°C Grade Count:4 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Asia Pacific) Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 80.0 °C |
0.335 BTU/lb-°F @Temperature 176 °F |
DSC |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry) Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Conditioned) Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3WG7 BK 00564 30% Glass Filled PA6 (Dry) Description: 35% glass-fiber reinforced and heat aging resistant injection-molding grade, e.g. for automotive manifolds and pedals.Information provided by BASF |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
Goodfellow Cellophane, Rayophane Regenerated Cellulose Fiber All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by.. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman VersaTray 12822 Plastic
(discontinued **) VersaTray plastic 12822 is a polyethylene terephthalate resin designed for use as a base resin for crystallized PET (CPET) food trays and other high temperature food packaging applications. CPET foo.. |
|||
Specific Heat Capacity | 1.40 J/g-°C @Temperature 100 °C |
0.335 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Conditioned) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |
|||
Specific Heat Capacity | 1.40 J/g-°C | 0.335 BTU/lb-°F | |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |