Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.30 J/g-°C | 0.310 BTU/lb-°F | |
Owens Corning Glass Fiber Reinforced Polyester (Spray-up/Lay-up), 30 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
Specific Heat Capacity | 1.30 J/g-°C @Temperature 80.0 °C |
0.311 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman Aqua 18696 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186.. |
|||
Specific Heat Capacity | 1.30 J/g-°C @Temperature 80.0 °C |
0.311 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Specific Heat Capacity | 1.30 J/g-°C @Temperature 80.0 °C |
0.311 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman 9663 PET
(discontinued **) VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers.. |
|||
Specific Heat Capacity | 1.30 J/g-°C @Temperature 80.0 °C |
0.311 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman 9921 PET Film
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Specific Heat Capacity | 1.30 J/g-°C @Temperature 80.0 °C |
0.311 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Specific Heat Capacity | 1.30 J/g-°C @Temperature 80.0 °C |
0.311 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman A12 PET
(discontinued **) Voridian Polymer A12 is currently produced to Eastman`s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer A12 is available i.. |
|||
Specific Heat Capacity | 1.30 J/g-°C @Temperature 80.0 °C |
0.311 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman GP800 PET
(discontinued **) Voridian PET GP800 is a general purpose polymer that is available in the European, Middle East and Africa region. This product is developed for optimal production of PET bottles, containers, and fil.. |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
Eastman Eastar GN101 PETG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | ASTM D3418 |
Solvay Specialty Polymers Hylar® 301F Polyvinylidene Fluoride (PVDF)
(Unverified Data**) High Melt Viscosity - Polymer for Non-Architectural Dispersion CoatingsInformation provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 1.30 - 1.50 J/g-°C | 0.311 - 0.359 BTU/lb-°F | DSC |
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hylar® 301F Polyvinylidene Fluoride (PVDF) Hylar® 301F is a high melt viscosity polyvinylidene fluoride (PVDF) powder used for non-architectural dispersion coatings.Features: High Viscosity; HomopolymerUses: Coating ApplicationsAdditiona.. |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
Eastman Eastar GN007 PETG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
BASF Ultramid® A3EG10 High Speed Information provided by BASF |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Conditioned) Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for.. |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Dry) Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for.. |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Conditioned) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
Azoty Tarnow™ TARNOFORM 300 MW4 POM Mineral filled injection molding grade based on Tarnoform 300 reinforced with 20% wollastonite; such a compound has high stiffness, dimensional stability and hardness combined with low shrinkage.Inf.. |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Conditioned) Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles.. |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Dry) Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles.. |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
Hippe PS Polystyrene Amorphous thermoplastic with brilliant surface. High hardness and stiffness, but brittle and susceptible to impact. Very good dielectric properties. Physiologically safe if it falls below a parti.. |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Specific Heat Capacity | 1.30 J/g-°C | 0.311 BTU/lb-°F | |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Specific Heat Capacity | 1.30 J/g-°C @Temperature 80.0 °C |
0.311 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman 5214A PET
(discontinued **) Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containe.. |
|||
Specific Heat Capacity | 1.30 J/g-°C @Temperature 80.0 °C |
0.311 BTU/lb-°F @Temperature 176 °F |
ASTM E1269 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Specific Heat Capacity | 1.30 - 1.50 J/g-°C | 0.311 - 0.359 BTU/lb-°F | Average value: 1.44 J/g-°C Grade Count:11 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |