BASF Ultramid® A3EG10 High Speed

Category Polymer , Thermoplastic , Nylon
Manufacturer BASF
Trade Name Ultramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® A3EG10 High Speed.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by BASF
Physical Properties Metric English Comments
Spiral Flow 30.0 cm

@Thickness 1.50 mm,
Temperature 80.0 °C
11.8 in

@Thickness 0.0591 in,
Temperature 176 °F
290/1000 Bar
43.0 cm

@Thickness 2.00 mm,
Temperature 80.0 °C
16.9 in

@Thickness 0.0787 in,
Temperature 176 °F
290/1000 Bar
Mechanical Properties Metric English Comments
Tensile Strength at Break 240 MPa
34800 psi
Elongation at Break 2.2 %
2.2 %
Tensile Modulus 16.4 GPa
2380 ksi
Charpy Impact Unnotched 10.0 J/cm²
47.6 ft-lb/in²
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
Thermal Properties Metric English Comments
Specific Heat Capacity 1.30 J/g-°C
0.311 BTU/lb-°F
Electrical Properties Metric English Comments
Volume Resistivity 6.50e+14 ohm-cm
6.50e+14 ohm-cm
Dielectric Constant 4.1

@Frequency 1.00e+6 Hz
4.1

@Frequency 1.00e+6 Hz
Dielectric Strength 22.0 kV/mm

@Temperature 100 °C
559 kV/in

@Temperature 212 °F
IEC 60243/1
40.0 kV/mm

@Temperature 50.0 °C
1020 kV/in

@Temperature 122 °F
IEC 60243/1
40.0 kV/mm

@Temperature 23.0 °C
1020 kV/in

@Temperature 73.4 °F
IEC 60243/1
Dissipation Factor 0.017
0.017
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Commercial Status Europe