| Category | Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced | 
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Eastman A12 PET
      
       (discontinued **).pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Bulk Density | 0.830 g/cc | 0.0300 lb/in³ | Poured; ASTM D1895 | 
| 0.890 g/cc | 0.0322 lb/in³ | Vibrated; ASTM D1895 | |
| Density | 1.40 g/cc | 0.0506 lb/in³ | Crystalline Density; ASTM D1505 | 
| Melt Density |           1.20           g/cc           @Temperature 285 °C  | 
                  0.0434           lb/in³           @Temperature 545 °F  | 
        ASTM D1238 | 
| Particle Size | 2500 µm | 2500 µm | Pellet Size | 
| Viscosity Measurement | 0.80 - 0.84 | 0.80 - 0.84 | Intrinsic; EMN-A-AC-G-V-1 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Heat of Fusion | 62.0 J/g | 26.7 BTU/lb | ASTM E793 | 
| Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 | 
|           1.30           J/g-°C           @Temperature 80.0 °C  | 
                  0.311           BTU/lb-°F           @Temperature 176 °F  | 
        ASTM E1269 | |
|           1.40           J/g-°C           @Temperature 100 °C  | 
                  0.335           BTU/lb-°F           @Temperature 212 °F  | 
        ASTM E1269 | |
|           1.80           J/g-°C           @Temperature 200 °C  | 
                  0.430           BTU/lb-°F           @Temperature 392 °F  | 
        ASTM E1269 | |
|           2.00           J/g-°C           @Temperature 280 °C  | 
                  0.478           BTU/lb-°F           @Temperature 536 °F  | 
        ASTM E1269 | |
| Melting Point | 243 °C | 469 °F | Crystalline Peak Melting Point; ASTM D3418 | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Acetaldehyde | <1ppm | TEPO-A-AN-G-GC-67 | 
| Color, CIE a* | -2.5 to 0.0 | VGAS-A-AN-G-RS-001 | 
| Color, CIE b* | -1.5 to 1.5 | VGAS-A-AN-G-RS-001 | 
| Color, CIE L* | 80 min | VGAS-A-AN-G-RS-001 | 
| Fines, wt%, max | 0.05 | CEPC-A-AN-G-PTM-10 | 
| Pellet Shape | Cubical |