Thermal Properties Metric English Comments
Melting Point 211 °C
412 °F
crystalline melting point; DSC
Honeywell Stretch-Vac® 2000 Heat-Stabilized Blown Film  (discontinued **)
Description: Stretch-Vac® 2000 is a pink tinted, high elongation, heat-stabilized blown film produced from modified polyamide resin. It is available in widths up to 80 inches as layflat tubing and..
Melting Point 211 °C
412 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET  (Unverified Data**)
Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t..
Melting Point 211 °C
412 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® 6646 NC010 TPC-ET  (Unverified Data**)
Hytrel® 6646 NC010 is a medium modulus grade with nominal hardness of 66D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like ..
Melting Point 211 °C
412 °F
crystalline melting point; ASTM D4591
Honeywell ACLAR® 11A (8.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Melting Point 211 °C
412 °F
crystalline melting point; ASTM D4591
Honeywell ACLAR® 11A (4.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Melting Point 211 °C
412 °F
crystalline melting point; ASTM D4591
Honeywell ACLAR® 11A (3.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Melting Point 211 °C
412 °F
crystalline melting point; ASTM D4591
Honeywell ACLAR® 11A (2.00 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Melting Point 211 °C
412 °F
crystalline melting point; ASTM D4591
Honeywell ACLAR® 11A (0.90 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Melting Point 211 °C
412 °F
crystalline melting point; ASTM D4591
Honeywell ACLAR® 11A(0.60 mil) CTFE Homopolymer, Barrier Film  (discontinued **)
Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell.
Melting Point 211 °C
412 °F
crystalline melting point; ASTM D4591
Honeywell ACLAR® Rx 160 CTFE Homopolymer, Barrier Film
Description: Aclar® Rx160 is a 0.60 mil (15 micron) PCTFE homopolymer, high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packag..
Melting Point 211 °C
412 °F
crystalline melting point; ASTM D4591
Honeywell ACLAR® Rx20E CTFE Homopolymer, Barrier Film
Description: ACLAR® Rx20Eis a .8 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipment.Inf..
Melting Point 211 °C
412 °F
crystalline melting point; ASTM D4591
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film
Description: ACLAR® SupRx 900 is a .9 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme..
Melting Point 211 °C
412 °F
crystalline melting point; ASTM D4591
Honeywell ACLAR® UltRx 2000 CTFE Homopolymer, Barrier Film
Description: ACLAR® UltRx 2000 is a 2 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipmen..
Melting Point 211 °C
412 °F
crystalline melting point; ASTM D4591
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film
Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme..
Melting Point 211 - 213 °C
412 - 415 °F
Indium Corp. Indalloy® 249 91.8Sn/3.4Ag/4.8Bi Lead-Free Solder Alloy
Board & component metallizations must be Pb-free. U.S. Patent 5,439,639 (ICA Licensed Sandia Patent)Information provided by the manufacturer, Indium Corporation.
Melting Point 211 °C
412 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® 6646 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
66 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Melting Point 211 °C
412 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® SC969 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers
Melting Point 211 °C
412 °F
ASTM D3418
Ashley Polymers Ashlene® 520BU Nylon 66
A general purpose Nylon 66 resin, black, utility grade.Data provided by the manufacturer
Melting Point 211 °C
412 °F
ASTM D789
Chem Polymer Chemlon 267 Nylon 6, Impact Modified
An extrusion grade copolymer nylon 6, providing good melt strength, impact, elongation, and flexibility. This grade provides excellent properties in most convoluted tubing or wire coating applicati..
Melting Point 211 °C
412 °F
ISO 11357-1,-3
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66  (discontinued **)
PA 6/66
Melting Point 211 °C
412 °F
crystalline melting point; DSC
Honeywell Stretch-Vac® Elastomax 1000 Heat-Stabilized Blown Film  (discontinued **)
Description: Capran® Elastomax 1000 is a pink tinted, heat-stabilized blown film produced from modified nylon resin. It is available in widths up to 80 inches as layflat tubing and 120 inches as s..
Copyright © lookpolymers.com All Rights Reserved