Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 169 °C | 336 °F | Crystallinity by DSC; ASTM D 3418 |
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer
(discontinued **) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Melting Point | 169 - 181 °C | 336 - 358 °F | TMA Melt Range |
Huntsman IROGRAN® PS 443-201 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Melting Point | 169 °C | 336 °F | DSC |
Solvay Specialty Polymers Ixan® PVS 706 Polyvinylidene Chloride (PVDC) PVDC ready-to-use premix. Ixan® PVS 706 is an PVDC-based blend designed for the extrusion of monofilaments used in fibers applications, chemical and abrasion resistance, and flame resistance. It .. |
|||
Melting Point | 169 °C | 336 °F | DSC |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Sol.. |
|||
Melting Point | 169 °C | 336 °F | DSC |
Solvay Specialty Polymers Solef® 42308 Polyvinylidene Fluoride (PVDF) Solef® 42308 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Solvay S.. |
|||
Melting Point | 169 °C | 336 °F | ASTM D3418 |
UBE UBESTA® 3030JI44 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: ultra flexible, low migrationInformation provided by UBE. |
|||
Melting Point | 169 °C | 336 °F | ISO 11357-3 |
ExxonMobil EXACT™ 8230 Plastomer for Polymer Modification Product Description: Exact 8230 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties. It is designed.. |
|||
Melting Point | 169 °C | 336 °F | ISO 3146 |
Eurostar Star L POM D36 POM, Injection Molded Star L POM D36 is Molybdenum Disulfide Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 169 °C | 336 °F | ISO 3146 |
Eurostar Star L POM D61 POM, Injection Molded Star L POM D61 is a PTFE/Silicone Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar. |
|||
Melting Point | 169 °C | 336 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BM 17 PA* Product description: Grilon BM 17 natural is a medium viscosity multi-polyamide with a low melting point. Grilon BM 17 natural has the following features: High flexibility and toughnessVery good ori.. |
|||
Melting Point | 169 °C | 336 °F | ASTM D3418 |
Arkema Group Pebax® 6333 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Melting Point | 169 °C | 336 °F | ISO 11357 |
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Melting Point | 169 °C | 336 °F | ISO 11357 |
Arkema Group Pebax® 6333 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Melting Point | 169 °C | 336 °F | (Dry) |
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
Melting Point | 169 °C | 336 °F | 10°C/min |
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
Melting Point | 169 °C | 336 °F | ISO 11357 |
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Melting Point | 169 °C | 336 °F | ASTM D3418 |
3M Dyneon™ PVDF 31508/0003 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 31508/0003 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. PVDF 31508/0003 also has a very low brittleness temperature, for.. |
|||
Melting Point | 169 °C | 336 °F | ASTM D3418 |
3M Dyneon™ PVDF 6108/0001 Polyvinylidene Fluoride Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Melting Point | 169 °C | 336 °F | 10K/min; ISO 3146 |
CENTROPLAST CENTROFLON Polyvinylidene fluoride This material has very good chemical and temperature resistance, with good slip characteristics. Its applications include pump wheels, flanges, valve bodies, and laboratory equipment.Information pr.. |
|||
Melting Point | 169 °C | 336 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 169 °C | 336 °F | 10°C/min |
Arkema Group Kynar® 1000 HDC N 118 PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1C,P.?E5.I.B.E.C,, ?(1.5-2.5)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, hig.. |
|||
Melting Point | 169 °C | 336 °F | ASTM D3418 |
3M Dyneon™ PVDF 31508/0001 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesInformation provided by Dyneon, A .. |
|||
Melting Point | 169 °C | 336 °F | ASTM D3418 |
3M Dyneon™ PVDF 31508/0009 Polyvinylidene Fluoride 3M™ Dyneon™ PVDF 31508/0009 is a flexible copolymer of VF2 and CTFE, exhibiting very low shrinkage and excellent impact resistance. Dyneon PVDF 31508/0009 also has a very low brittleness temperatu.. |
|||
Melting Point | 169 - 172 °C | 336 - 342 °F | |
BASF 2,3,5-Trimethylhydroquinone Formula: C9H12O2CAS: 700-13-0Description: TMHQ is a colorless fine crystalline powder. It is insoluble in water, soluble in methanol, ethanol, diethyl ether, and acetone.Synonyms: TMHQ, TMHApplicat.. |