Material Notes:
Product description: Grilon BM 17 natural is a medium viscosity multi-polyamide with a low melting point. Grilon BM 17 natural has the following features: High flexibility and toughnessVery good orientation and thermoforming propertiesHigh shrinkageVery good transparencyLow melting point (169°C)Low glass transition point (43°C) Application Examples: Grilon BM 17 natural has been specially developed for cast and blown films coextruded with temperature sensitive polymers (PVDC, EVOH). Grilon BM 17 natural is suitable for flexible packaging for foodstuffs e.g. (shrinkable) film for consumer packaging of meat, cheese, sausage or fish.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183
Water Absorption 10 %
10 %
ISO 62
Moisture Absorption 3.00 %
3.00 %
ISO 62
Water Vapor Transmission 15.0 g/m²/day
0.966 g/100 in²/day
23°C/85%r.h.; DIS 15106-1/-2
Oxygen Transmission Rate 75.0 cc/m²/day
4.83 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
110 cc/m²/day
7.08 cc/100 in²/day
23°C/0%r.h.; DIS 15105-1/-2
Carbon Dioxide Transmission 275 cc-mm/m²-24hr-atm
699 cc-mil/100 in²-24hr-atm
23°C/0%r.h.; DIS 15105-1/-2
290 cc-mm/m²-24hr-atm
737 cc-mil/100 in²-24hr-atm
23°C/85%r.h.; DIS 15105-1/-2
Melt Flow 100 g/10 min
100 g/10 min
(MVR) [cm³/10min]; ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 25.0 MPa
3630 psi
ISO 527-3
Film Tensile Strength at Yield, TD 25.0 MPa
3630 psi
ISO 527-3
Film Elongation at Break, MD 400 %
400 %
ISO 527-3
Film Elongation at Break, TD 400 %
400 %
ISO 527-3
Film Elongation at Yield, MD 7.0 %
7.0 %
ISO 527-3
Film Elongation at Yield, TD 6.0 %
6.0 %
ISO 527-3
Tensile Modulus 0.650 GPa
94.3 ksi
conditioned; ISO 527-1/-2
Coefficient of Friction, Dynamic 0.80
0.80
ISO 8295
Film Tensile Strength at Break, MD 70.0 MPa
10200 psi
ISO 527-3
Film Tensile Strength at Break, TD 60.0 MPa
8700 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 169 °C
336 °F
10°C/min; ISO 11357-1/-3
Optical Properties Metric English Comments
Haze 19 %
19 %
ISO 14782
Gloss 64 %
64 %
60°; ISO 2813
Descriptive Properties Value Comments
Food contact EU Requirements
Form Granules
Packaging Non oriented film
Oriented film
Paper coating
Processing Blown Film Extrusion
Film Extrusion
Other Extrusion
Product Attributes Barrier Properties
Co Polyamide
High viscosity
Special Characteristics Transparent
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved