Solvay Specialty Polymers Solef® 42308 Polyvinylidene Fluoride (PVDF)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer Solvay Specialty Polymers
Trade Name Solef®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Specialty Polymers Solef® 42308 Polyvinylidene Fluoride (PVDF).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Solef® 42308 PVDF is specifically developed for coextrusion.Additional Properties: Crystallization Heat - ASTM D3418 51.6 J/g; Heat of Fusion - ASTM D3418 52.7 J/gInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ISO 1183
Water Absorption <= 0.040 %

@Time 86400 sec
<= 0.040 %

@Time 24.0 hour
ISO 62
Melt Flow 6.0 - 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
6.0 - 8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
18 - 24 g/10 min

@Load 5.00 kg,
Temperature 230 °C
18 - 24 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 48.0 MPa
6960 psi
50 mm/min; ASTM D638
Elongation at Yield 7.0 %
7.0 %
50 mm/min; ASTM D638
Tensile Modulus 1.90 GPa
276 ksi
1.0 mm/min; ASTM D638
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179
Coefficient of Friction, Dynamic 0.31
0.31
vs. Itself; ASTM D1894
Coefficient of Friction, Static 0.32
0.32
vs. Itself; ASTM D1894
Taber Abrasion, mg/1000 Cycles 8.0
8.0
CS-10 Wheel, 1000 g; ASTM D1044
Thermal Properties Metric English Comments
Melting Point 169 °C
336 °F
DSC
Crystallization Temperature 136 °C
277 °F
Peak; ASTM D3418
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
ASTM D257
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Processing Technique Coextrusion