Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa SINKRAL B23 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-25 High heat resistant grade with good impact resistance. Suitable for injection moulding and extrusi.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa SINKRAL C333/m² ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-20 Special low gloss grade for injection moulding which combines medium heat resistance with a good b.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa SINKRAL G320 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-25 General purpose injection moulding grade with good impact resistance, good flow and high gloss. SI.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa SINKRAL PD H330/S ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-25 Injection moulding grade with high flow and gloss, specially developed to meet the requirements of.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® F223-DH (Dry) Low/Medium Viscosity, Heat Stabilized Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® B 30 S FN40 000000 Nylon 6 PA 6, injection molding grade, non- reinforced, good flowability, easy-release, fast cycling, UL 94V-2 off 0,75 mm, GWIT 775°C bei 0,75/1,5mm |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 7062 PBT+PET (Europe-Africa-Middle East) Valox 7062 is Mineral filled PBT injection molding grade. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® POM CO TL15 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL HF185 PPE+HIPS (Europe-Africa-Middle East) NORYL HF185 is an unfilled, halogen free (according VDE/DIN 472 part 815), flame retardant and easy flow NORYL grade. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Europe-Africa-Middle East) NORYL* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade, targeted for flat panel TV enclosures. It has a Vicat B/120 temperature of 96 degC and UL-94 V0 @ 1.5mm .. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® T 45 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
DSM Akulon® F136-C1 PA6 Very High Viscosity, Film Extrusion, Lubricated |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
DSM Akulon® F234-C PA6 Film Extrusion, High Viscosity, Lubricated |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Akulon® F-X9182 PA6 Low/Medium Viscosity |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Novamid® ST120 NAT PA6-I Impact Modified, Injection Molding |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GM-4H PA*-MD40 Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 3997 nat PAMACM12 Product description: Grilamid XE 3997 natural is a transparent thermoplastic polyamide based on aliphatic and cycloaliphatic blocks. Grilamid XE 3997 natural is particularly suitable for blow molded.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BK-30 PA6-GB30 Information provided by EMS Grivory |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BRZ 340 H PA6 Product description: Grilon BRZ 340 H is a heat stabilized, high viscosity, impact modified PA6 extrusion grade. Grilon BRZ 340 H has the following important properties:High impact strength at low t.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Prevail® 3100 ABS + Polyurethane PREVAIL® 3100 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Conditioned) Designation ISO 1874-PA12,MHLS,14-010,MD05Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient. Goo.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® D 1118 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® FG151L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | >= 90.0 µm/m-°C | >= 50.0 µin/in-°F | |
BASF Ultramid® B3UG4 LS Grey 22985 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® 452
(discontinued **) Key Features:UnfilledSuitable processing methods:Sheet extrusionThermoformingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after I.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa SINKRAL D160 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,115-08-09-25 Very high heat injection moulding grade with good flow. Permits production of complex, thin walled.. |