Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Flexible Tubing Grade
Manufacturer Arkema
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI approval.Example applications: Catheters.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
Melt Flow 15.5 g/10 min

@Load 2.16 kg,
Temperature 235 °C
15.5 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.0 MPa

@Strain 50.0 %
2320 psi

@Strain 50.0 %
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Tensile Modulus 0.180 GPa
26.1 ksi
1 mm/min
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Melting Point 150 °C
302 °F
(Dry)
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C
156 °F
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °C
106 °F
Vicat Softening Point 180 °C
356 °F
50°C/hr; 50N
Flammability, UL94 V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Electrical Properties Metric English Comments
Electrical Resistivity 6.00e+10 ohm-cm
6.00e+10 ohm-cm
Surface Resistance 4.00e+13 ohm
4.00e+13 ohm
Dielectric Strength 32.0 kV/mm
813 kV/in