Material Notes:
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-25 General purpose injection moulding grade with good impact resistance, good flow and high gloss. SINKRAL G320 is widely used for applications in the telecommunications industry, office equipment, electrical tools and consumer goods.Unfilled. Suitable for Injection Molding. Supplied as pellets. Contains lubricant and release agent.ISO data except as noted. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 1.0 %
1.0 %
Moisture Absorption at Equilibrium 0.20 %
0.20 %
Humidity Absorption
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Cond. I; ASTM D1238
18 g/10 min

@Load 10.0 kg,
Temperature 220 °C
18 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 46.0 MPa
6670 psi
50 mm/min
Elongation at Break 10 %
10 %
Nominal
Elongation at Yield 3.1 %
3.1 %
50 mm/min
Tensile Modulus 2.35 GPa
341 ksi
1 mm/min
Flexural Modulus 2.55 GPa
370 ksi
ASTM D790
Izod Impact, Notched 3.50 J/cm

@Thickness 3.17 mm
6.56 ft-lb/in

@Thickness 0.125 in
ASTM D256
Charpy Impact Unnotched 16.0 J/cm²
76.1 ft-lb/in²
11.0 J/cm²

@Temperature -30.0 °C
52.4 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Vicat Softening Point 98.0 °C
208 °F
50°C/hr; 50N
Glass Transition Temp, Tg 105 °C
221 °F
10°C/min test
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.10 mm
HB

@Thickness 0.122 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Constant 3.0

@Frequency 1e+6 Hz
3.0

@Frequency 1e+6 Hz
3.2

@Frequency 100 Hz
3.2

@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm
762 kV/in
Dissipation Factor 0.0080

@Frequency 1e+6 Hz
0.0080

@Frequency 1e+6 Hz
0.015

@Frequency 100 Hz
0.015

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V