Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® HMG47MD ABS General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38F ABS Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38F ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG47 ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG47F ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG47F ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG47N ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG47N ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MG94 ABS (Asia Pacific) Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MGABS01 ABS Injection molding ABS. High impact, high gloss, good flow. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® MGABS02 ABS General purpose ABS. Excellent flow/impact. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 LNP* STAT-KON* SE003 is a compound based on Nylon 12 resin containing 15% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
49.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Asia Pacific) LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C | 49.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE TM20 20% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C | 49.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE TM20 UV BK 20% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: BlackInformation provided by TP Composi.. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C | 49.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE TM25 25% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 25% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C | 49.0 µin/in-°F | Length |
Saint-Gobain Rulon® 142 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
CTE, linear, Parallel to Flow | 88.2 µm/m-°C @Temperature 20.0 °C |
49.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PlastxWorld CEVIAN®-V 320 ABS High Impact ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |