Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ 80510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnite® CCT GF30 (T-X01301) PBT-30% Glass Reinforced (European Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1,-2 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1,-2 |
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers PA 6-Copolymer, 15% glass fibers, injection molding, impact modified |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Pocan® B 3216 HR 000000 PBT 16% Glass Fiber PBT, 16% glass fibers, injection molding, improved impact strength, hydrolysis stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® BF 4215 000000 PBT, 12% Glass Fiber PBT, 12% glass fibers, injection molding, flame retardant |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® KU 1-7625 901510 PBT + PC, 20% Glass Fiber PBT+PC, 20% glass fibers, injection molding, low tendency to warp, improved surface finish |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
22.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL ZWM2411 PPE+PS (Asia Pacific) Modified PPO*, 30% mineral filled product, V-1@1.5mm, HDT 125degC, low warpage product, BK color only |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 LNP THERMOCOMP* RF00C is a compound based on Nylon 66 resin containing 60% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
Covestro Bayblend® T90 MF-20* Polycarbonate + ABS, Mineral Filled Developmental productInjection molding grade20 % mineral filledvery good flowreduced coefficient of thermal dilatationtensile modulus = 5200 MPaVicat/B 120 = 130 °CPreprocessingMax. Water content |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K223-HM6 (BLACK) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TV4 241 SN PBT-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Arnite® TV4 270 PBT-35% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® B 70 GFE 15 H PA6-GF15 Product description: Grilon B 70 GFE 15 H is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon B 70 GFE 15 H has the following important prop.. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BGZ-15 PA6-GF15 Information provided by EMS Grivory |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Stanyl® TE250F3 Nylon 46-15% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LV-2A NZ PA12-GF20 Product description: Grilamid LV-2A NZ is a high viscosity polyamide 12 with 20% glass fibers and improved hydrolysis resistance compared to standard polyamide 12 materials. Grilamid LV-2A NZ has a .. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RB006S PA66, 30% Glass Bead Filled, Injection Molded Staramide RB006S is a 30% Glass Bead Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S3)Information provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 20.0 °C |
22.2 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-HM8 Nylon 66-40% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBATER BF250 PBT, 50% glass fiber reinforced, food grade PBT-GF50Information provided by BARLOG plastics GmbH. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ASTM E 831 |
Arlon Thermabond® 48991A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation IIa Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style .. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ASTM E 831 |
Arlon Thermabond® 48991A015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Thermabond® G2pr - electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 Fiberg.. |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C | 22.2 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TZ6 280 PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
CTE, linear, Parallel to Flow | 40.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East) VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 40.0 - 50.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
22.2 - 27.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |