Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature -40.0 - 60.0 °C |
75.0 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® BDT5510 ABS Automotive. High heat resistance, low gloss, color concentratable for interior applications. Natural only. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
Covestro Baydur® GS PUR Polyurethane Polyurethane casting system for the production of solid components. Pressureless casting into open or closed molds, fast demold times, good rot resistance. Combines easily with other materials.Infor.. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1040 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1040 RC Polypropylene, Injection Molding Grade Injection moldingsData was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1100 H Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1100 L Polypropylene, Injection Molding Grade Injection molded parts, film tape, fibrillated film and monofilaments.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1100 UC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1101 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1101 P Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1101 R Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1102 G Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1102 H Polypropylene Grade with high processing stability for packaging tapes, film tape, fibrillated film, monofilaments, thermoformed and blow molded parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1184 L Polypropylene Nucleated grade with high processing stability containing antistatic for thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1102 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1100 N Polypropylene, Injection Molding Grade Grade for injection molded parts. Also available as a special grade for fibers (short spinning) and cast film.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1100 VC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1101 N Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1102 J Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1102 K Polypropylene Grade with high processing stability for film tape (low water carryover), fibrillated film, monofilaments, OPP film (special formulations) and thermoformed parts.Data was collected by ISO methods an.. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1102 L Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1104 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1125 N Polypropylene Cast film with medium slip.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1126 N Polypropylene Grade with slip and antiblocking agents, for cast and water-cooled blown film with very good slip and especially low tendency to block.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1127 N Polypropylene Grade with slip and antiblocking agents, for cast film; with very good slip.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1148 RC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1148 TC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Novolen® 1148 UC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
ASTM D636 |
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Load-bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product line from Dow in.. |
|||
CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 525-10 CAB Cellulose Acetate Butyrate