Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Murtfeldt Muralen® Black Antistatic Polyethylene, Conductive Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Murtfeldt Muralen® plus + AB Polyethylene, Antibacterial Muralen® is based on high molecular weight polyethylene (PE-HMW) and is ideally suited for use in applications that require the generally impressive material properties of polyethylene. Because of.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Cast Nylon 6, Glass Filled Information provided by Nylacast Ltd. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Impact Nylon 6, Impact Grade Nylacast Impact has been designed for applications that have a high impact resistance and noise reduction capabilities. It works more effectively in applications where there are high stress. It also.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Moly Cast Nylon 6, MoS2 Filled Nylacast Moly is part of the Cast Nylon 6 family. Its improved crystallization occurs by the addition of Molybdenum Disulphide. It includes MoS2, which is an extremely effective self dry lubricant w.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Nylube GF Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), Glass Filled For applications requiring higher compressive strength the NYLUBE GF masterbatch incorporates hollow glass ovule, designed to float and evenly distribute through the polymerising polymer. The glass .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled The combined Nylube lubrication system incorporating fine particles of molybdenum disulphide provides enhanced load bearing capabilities while retaining Nylube's excellent frictional characteristics.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Nylacast Oilon Cast Nylon 6, Lubricated (Lubricant Oil Filled) This exceptional oil-loaded nylon features a complex blended oil lubrication system, uniformly distributed throughout the product, that guarantees constant performance over the whole service life. E.. |
|||
Minimum Service Temperature, Air | -100 - -40.0 °C | -148 - -40.0 °F | Average value: -55.0 °C Grade Count:3 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Global EPP PA 6C Cast Polyamide 6 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Global EPP PA 6C MOLY Cast Polyamide 6 + MoS2 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Global EPP PA 6C OFN Cast Polyamide 6 + Blended Liquid Lubricant Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Continuous |
Isoflon FEP Fluorinated Ethylene Propylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Intermittent |
Lord Adhesives Circalokâ„¢ 6715 Silicone Encapsulant Circalokâ„¢ 6715 is a two component, medium viscosity, solvent-free silicone which cures at room temperature to an elastomeric, stress-free rubber of outstanding electrical and high temperature p.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Shin-Etsu Silicones KE-5006BU Low Temperature Silicone Elastomer ShinEtsu KE5006B U is a phenyl (PVMQ) silicone compound. This product is designed for good low temperature characteristics.Product Features: A broad range of service temperatures from 100 to +260°.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Shin-Etsu Silicones X-30-1028U Low Temperature Silicone Elastomer ShinEtsu X301028U is a phenyl (PVMQ) silicone base. This product is designed for good low temperature characteristics. Product Features: A broad range of service temperatures from 100 to +260°C (.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Shin-Etsu Silicones X-30-783U Silicone Elastomer ShinEtsu X30783 U is a phenyl (PVMQ) silicone product. This product is designed for good low temperature characteristics. Product Features: A broad range of service temperatures from 100 to +260°.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Zeus ETFE Tubing ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Adalon® 203 PTFE, 15/5% Glass/Graphite Filled Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Adalon® 807 PTFE, 40% Bronze + 5 MoS2 Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Adalon® 817 PTFE, 60% Bronze Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon CP-594CX Bulk Compound Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Gray, high viscosity gumUL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but .. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon Thermabond®-II 99760N008 0.008" (0.203 mm) Unsupported/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Unsupported/Uncured RubberAppearance: White/gray gumAppearance: White/grey gumThis data Represents typical values for the production material. The data should not be used.. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Adalon® 816 PTFE, 46% Bronze, Blue Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | DSC |
Adamas Rixon U PEEK, Unreinforced Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | Continuous |
Isoflon ETFE Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Minimum Service Temperature, Air | -100 °C | -148 °F | |
Arlon R37806X030 Silicone Rubber/Fiberglass Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |