Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 3.16 - 3.20 g/cc
3.16 - 3.20 g/cc
ASTM D792
Deformation 7.0 - 10 %
7.0 - 10 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 58 - 62
58 - 62
ASTM D2240
Ball Indentation Hardness 48.0 - 52.0 MPa
6960 - 7540 psi
ISO 2032
Tensile Strength at Break >= 20.0 MPa
>= 2900 psi
ISO 527-1
Elongation at Break >= 200 %
>= 200 %
ISO 527-1
Coefficient of Friction, Dynamic 0.14 - 0.16
0.14 - 0.16
ASTM D1894
Coefficient of Friction, Static 0.16 - 0.18
0.16 - 0.18
ASTM D1894
Thermal Properties Metric English Comments
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
DSC
Minimum Service Temperature, Air -100 °C
-148 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 ohm-cm
1.00e+7 ohm-cm
ASTM D257