Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 120 °C @Load 5.001 kg |
248 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYblend 85VB PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Vicat Softening Point | 120 °C @Load 5.001 kg |
248 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYlux 4010 MP PC/PBT-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® ML1010 PC (Europe-Africa-Middle East) Superior performance, improved flow over standard grades at lower temperatures. Internal mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D 1525 |
Ineos K38-20X2091 HDPE K38-20X2091 is a yellow medium density polyethylene resin designed specifically for natural gas pipe extrusion. It exhibits excellent long term stress life and slow crack growth resistance. This m.. |
|||
Vicat Softening Point | 120 °C | 248 °F | 50°C/h 50N; ISO 306 |
Mitsubishi Xantar® C CM 406 FD Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Vicat Softening Point | 120 °C | 248 °F | VST/B/50; ISO 306 |
Styrolution Luran® S KR 2864 C Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Unannealed; ISO R 306 |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Vicat Softening Point | 120 °C | 248 °F | (50 °C/h / 50N) - B/50; ISO 306 |
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Dry) Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Unannealed; ISO R 306 |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
SK Chemicals SKYTHANE® S360D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
Styron MAGNUMâ„¢ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL IN120 PPE+HIPS (Europe-Africa-Middle East) NORYL IN120 is an unfilled material with a Vicat B/120 of 125 °C according ISO 306. NORYL IN120 has been developed for the interior automotive |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL N110S PPE+HIPS (Europe-Africa-Middle East) NORYL N110S is an unfilled material with a Vicat B/120 of 115 ?C according ISO 306. NORYL N110S cust spec 1977 has been listed for potable water |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL PX1185 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1185 is a special NORYL grade developed for extrusion of automotive trims. NORYL PX1185 offers high heat resistance and good impact performance. |
|||
Vicat Softening Point | 120 °C | 248 °F | A50 (10 N); ISO 306 |
Borealis Borcoat™ HE3453 Natural High Density Polyethylene for Steel Pipe Coating Borcoat HE3453 is a natural and colorable high density polyethylene produced with the Borstar technology in similar conditions as the black ready made top coat Borcoat HE3450. Borcoat HE3453 is rec.. |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM-D1525 |
Polyram RamLloy PBB702 PC/ABS alloy, UV Stabilized UV stabilized PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
Toyobo PELPRENE™ P40H Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Vicat Softening Point | 120 °C @Load 5.00 kg |
248 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTAPROP H 0560 GF Polypropylene, 30% Glass Filled PP homopolymer 30% glass fiber reinforcedGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 120 °C | 248 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ASA/PC FA-30 Description: ASA Weatherable Polymer, Injection Molding Grade, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 120 °C @Load 5.00 kg |
248 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTAPROP KUR 1060 GFC Polypropylene, 30% Glass Filled PP copolymer 30% chemically coupled glass fiberElastomer modified, good impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate A (50°C/h), Loading 1 (10 N); ASTM D1525 |
Entec Hypel® PEHD30/.950 HDPE Available in North America Features: High DensityRoHS Compliant Form: Pellets Information provided by Entec |
|||
Vicat Softening Point | 120 °C | 248 °F | |
Arkema Group Orevac® 18732 RBP Maleic Anhydride modified Polypropylene PP base Structure: Repairing and joint Applications: Pipe CoatingInformation provided by Arkema Group |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR4525 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron IMC-45M ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Vicat Softening Point | 120 °C @Load 1.00 kg, Thickness 4.00 mm |
248 °F @Load 2.20 lb, Thickness 0.157 in |
ISO 306 |
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Vicat Softening Point | 120 °C | 248 °F | Rate A/120; ISO 306 |
SABIC Innovative Plastics Cycolac® DL100LG ABS (Europe-Africa-Middle East) Cycolac DL100LG is a low gloss, high heat, high impact ABS/PC blend with low emission |
|||
Vicat Softening Point | 120 °C | 248 °F | ASTM D1525 |
NOVA Chemicals Sclair® 2715 HDPE Injection Molding Resin
(discontinued **) Features: Excellent low temperature impact strength, good balance of toughness and stiffness, low odor.Applications: Thin walled food containers and lids, frozen and refrigerated containers.Data pro.. |