Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 113 °C | 235 °F | ASTM D-1525 |
Plaskolite Optix® CA - 75 OG General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Vicat Softening Point | 113 °C @Load 1.00 kg |
235 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® RN 50 U Linear Medium Density Polyethylene Clearflex RN 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha.. |
|||
Vicat Softening Point | 113 °C @Load 1.00 kg |
235 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® RP 50 U Linear Medium Density Polyethylene Clearflex RP 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RP 50 U show good mecha.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycolac® GRM2600L ABS High Impact , good chemical resistance sheet grade ABS designed for refrigerator liner applications. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® C1000 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1000 is a PC+ABS blend developed with emphasis on excellent processing efficiency while maintaining good heat resistance and impact ductility. It is an excellent material choice for a wide .. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate A; 4 mm thick;10.0 mm wide molded rod; ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® ESD 7200 PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for inj.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Europe-Africa-Middle East) Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Asia Pacific) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® XP7560 ASA (Europe-Africa-Middle East) GELOY XP7560 is a general purpose ASA/PC injection moulding grade, available in various colours. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Vicat Softening Point | 113 °C | 235 °F | 50°C/hr; 50N |
Polimeri Europa KOBLEND HI PD 14 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend, similar to KOBLEND HI 18 with higher shrinkage values. Main application fields: bumpersUnfilled. Suitable for Injection .. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific) DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r.. |
|||
Vicat Softening Point | 113 °C | 235 °F | 1 kg; ASTM D1525 |
LG Chemical IH830C PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |
|||
Vicat Softening Point | 113 °C @Load 5.00 kg |
235 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical XR490 ABS, Heat Resistance, Low Emission Feature: Injection Molding, Heat Resistance, Low EmissionApplication: Automotives Interior Housing (Glove Box Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG C.. |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D1525 |
Lushan L-5R (F) Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS LNP LUBRICOMP* NL001 is a compound b ased on PC+ABS resin containing 5% PTFE. Added features include: Wear Resistant, Suitable for Thin Wall Applications. |
|||
Vicat Softening Point | 113 °C | 235 °F | VST/A/50; ISO 306 |
Styrolution Luran® S 778 TE Black 25991 ASA Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Vicat Softening Point | 113 °C | 235 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® SR-0325LTS ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 113 °C @Thickness 3.17 mm |
235 °F @Thickness 0.125 in |
50°C/hr; ASTM D1525 |
Chi Mei Kibilac® PW-978B ASA, High Heat Acrylonitrile/Styrene/AcrylateInformation provided by Calsak Corporation |
|||
Vicat Softening Point | 113 °C | 235 °F | 50N; ISO 306 |
Denka MALECCA K-100 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D1525 |
Dow DOWLEX™ 2025G Linear Low Density Polyethylene DOWLEX™ 2025G is a medium modulus resin with excellent toughness properties designed for thin film applications.Information provided by Dow |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D1525 |
Engineered Plastics EP Alloy 510B PC/ABS Alloy Gray. Stiff tough and excellent color stability. Used in housings for computers, printers, copiers and for auto parts such as air ducts and instrument panels. GMP # 002; Ford # WSS585. Propert.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron KU-600 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D1525 |
NOVA Chemicals Novapol® TR-0535-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |