Chi Mei Kibilac® PW-978B ASA, High Heat

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer Chi Mei Corporation (ChiMei)
Trade Name Kibilac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chi Mei Kibilac® PW-978B ASA, High Heat.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Acrylonitrile/Styrene/AcrylateInformation provided by Calsak Corporation
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa

@Thickness 3.17 mm
6530 psi

@Thickness 0.125 in
6 mm/min; ASTM D638
Flexural Yield Strength 72.4 MPa

@Thickness 6.35 mm
10500 psi

@Thickness 0.250 in
2.8 mm/min; ASTM D790
Izod Impact, Notched 1.49 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.80 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
2.46 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
4.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 39.4 °C
103 °F
annealed, unspecified pressure; ASTM D648
92.8 °C
199 °F
unannealed, unspecified pressure; ASTM D648
Vicat Softening Point 113 °C

@Thickness 3.17 mm
235 °F

@Thickness 0.125 in
50°C/hr; ASTM D1525
Optical Properties Metric English Comments
Gloss 96 %
96 %
ASTM D523