Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 41 FDA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 90.0 °C @Load 1.00 kg |
194 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FH 10 Low Density Polyethylene - Blown Film Extrusion Riblene FH 10 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 10 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CY6009 PC+ABS (Asia Pacific) CY6009 is a flame retardant (FR) PC+ABS blend with non-brominated and non-chlorinated FR systems. Its excellent flow together with balanced properties and thin wall 5VB capability at less than 2 mm.. |
|||
Vicat Softening Point | 90.0 - 95.0 °C | 194 - 203 °F | Average value: 92.7 °C Grade Count:3 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
LyondellBasell Petrothene® NA420127 Low Density Polyethylene
(discontinued **) ApplicationsPETROTHENE NA 420 is a LDPE/EVA copolymer resin for high impact and clarity packaging film. This resin exhibits excellent processability over a broad range of extrusion conditions. Wel.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | molding; ASTM D1525 |
LyondellBasell Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade Petrothene NA967000 is a low density polyethylene resin designed for blown film, general purpose and industrial packaging applications. NA967000 exhibits good processing characteristics and impact s.. |
|||
Vicat Softening Point | 90.0 °C @Load 5.00 kg |
194 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical TR300 MABS, Flame Retardant, Transparency Feature: Injection Molding, Flame Retardant, TransparencyApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9010-94-0 and 25713-60-4Information provided by LG Ch.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
LyondellBasell Petrothene® NA426225 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA426 is a series of LDPE/EVA copolymer resins for high impact and clarity packaging film. These resins exhibit excellent a broad range of extrusion conditions. Well-balanced films with e.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Noryl V190 PPE+HIPS (Europe-Africa-Middle East) NORYL V190 is an unfilled flame retardant material with a Vicat B/120 of 90°C according ISO 306. NORYL V190 is V1 at 2.0 mm according UL94 and halogen free according VDE/DIN 472 part 815.This dat.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® VE-0558 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | Unannealed; ISO R 306 |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Vicat Softening Point | 90.0 °C | 194 °F | VST/B/50; ISO 306 |
Styrolution Terluran® SP-6 ABS Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Vicat Softening Point | 90.0 °C | 194 °F | Unannealed; ISO R 306 |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
SK Chemicals SKYTHANE® S195A C series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Noryl N750T PPE+HIPS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Teknor Apex Sinvicomp SRP 5906 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Medium Impact Resistance Uses: Conduit; Piping; Profiles Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ISO 306 |
Total LDPE LA 0710 Low Density Polyethylene - Extrusion Coating LDPE LA 0710 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum. High draw down, low neck in.In.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | 50N-50°C per hour; ISO 306 |
Total PPH 10042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 10042 is a nucleated antistatic homopolymer. PPH 10042 is characterized by high fluidity for high speed injection of thin wall articles such as dairy pots and tubs, salad .. |
|||
Vicat Softening Point | 90.0 °C @Load 5.10 kg |
194 °F @Load 11.2 lb |
50°C per hour; ISO 306B50 |
Total PS CPDS FT875 Flame Retardant Polystyrene POLYSTYRENE (PS) COMPOUND (CPDS) FT875 is a high impact, halogen free flame retardant polystyrene. PS CPDS FT875 offers high heat stability and is recommended for the manufacturing of articles whic.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
ExxonMobil LD 144.50 Packaging Film Resin Film made from LD 144.50 offers improved impact strength and heat sealability compared to homopolymer clarity film resins. Typically applications include food packaging, frozen food packaging, and .. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | |
BASF Polystyrol® 476 L Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade. When extruded it is often mixed with PS 165 H.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ISO 306 |
Arkema Group OREVAC® 18365 Maleic Anhydride Modified Polyethylene OREVAC® 18365 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | 50°C/h 50N; ISO 306 |
DSM Arnitel® UM551-V 55 Shore D, Flame Retardant (halogen-, phosphorous-free) Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | 50°C/h 50N; ISO 306 |
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)
(discontinued * Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Huntsman PE1403 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA Copolymer, DMF listed and FDA compliantFeatures: High clarity film with good toughness and flexibility at low temperatures.Applications: Film extrusion: frozen food and general .. |
|||
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
PlastxWorld CEVIAN® SER20 ABS General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat.. |