Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 230 °C | 446 °F | STN EN ISO 306 |
Plastcom SLOVAMID® 6 GF 20 FRA 5 PA6 reinforced with glass fiber, flame retarded PA 6 for injection molding, reinforced with 20% glass fiber, flame retarded with halogen flame retardant. Main features: flammability in accordance with UL 94 5 at 1.6 mm, glow wire at 960°C. Appli.. |
|||
Vicat Softening Point | >= 230 °C @Load 5.001 kg |
>= 446 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANAMID 66 A12^ F30 TF15 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Vicat Softening Point | 230 - 255 °C | 446 - 491 °F | Average value: 246 °C Grade Count:7 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Vicat Softening Point | >= 230 °C | >= 446 °F | 50 N; ISO 306 |
Grupo Repol Dinalon® A1S25 G25PV0 25% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 66 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Vicat Softening Point | >= 230 °C | >= 446 °F | 50N; ISO 306 |
Grupo Repol Dinalon® A1S25 G30XV0 PA66 30% Glass Fiber V0 Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Vicat Softening Point | >= 230 °C | >= 446 °F | 50N; ISO 306 |
Grupo Repol Dinalon® A1S25 G35 H PA66 35% Glass Fiber, Heat Stabilized Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Vicat Softening Point | 230 °C | 446 °F | 50°C/h 50N; ISO 306 |
Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: gearbox oil sumps, oil modules |
|||
Vicat Softening Point | 230 °C | 446 °F | 50°C/h 50N; ISO 306 |
Lanxess Durethan® AKV 35 H3.0 000000 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistance |
|||
Vicat Softening Point | 230 °C @Load 5.10 kg |
446 °F @Load 11.2 lb |
120°C/hour; ISO 306 |
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66 PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS. |
|||
Vicat Softening Point | 230 °C | 446 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1-3260/schwarz Polyamide 66, with PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Vicat Softening Point | 230 °C | 446 °F | 50°C/h 50N; ISO 306 |
Lanxess Durethan® A 30 000000 Nylon 66 PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidificationApplication Examples: terminal blocks, cable clips, bobbins, gearwheels |
|||
Vicat Softening Point | 230 °C @Load 5.10 kg |
446 °F @Load 11.2 lb |
120°C/hour; ISO 306 |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Vicat Softening Point | 230 °C | 446 °F | 50°C/h 50N; ISO 306 |
Lanxess Durethan® AKV 15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, injection molding grade, 15% glass fibers, good heat-ageing resistance |
|||
Vicat Softening Point | 230 °C | 446 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Ultem PW2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
Vicat Softening Point | 230 °C | 446 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 CF10 HWCP 10% Carbon Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 CF20 HWCP 20% Carbon Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 GV 25 HWCP 25% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 GV 5 HWCP 5% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 HWUVCP Nylon 66, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 MF30 HWCP 30% Milled Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 MZ 401 CP Combination Nylon 66, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600/50 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | B/120; ISO 306 |
Eurostar Staramide BK8 PA6, 40% Mineral Fiber Filled, Injection Molded Staramide BK8 is a 40% Mineral Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 GS 40 HWCP 40% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6600 MR 409 HWCP 40% Mineral Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 230 °C | 446 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Valox® V9230CS PET (Europe-Africa-Middle East) 15% GF PET Injection Moulding grade, Heat and Color Stabilised, for light colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 230 °C | 446 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1-7497 Polyamide 66, with PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |