Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 161 °C | 322 °F | ASTM D1525 |
Multibase Nylex™ 2185 HFX Natural Polyamide + PP Forms: PelletsProcessing Methods:Injection moldingFeatures:Tensile Strength, HighInformation provided by Multibase |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East) XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL TN300 PPE+PS PPE+PS. Transparent. High heat. Color Limited. Injection molding. Laser-Transmission welding applications. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ325 PBT (Asia Pacific) PBT resin, using chemically recycled post consumer PET Bottles. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Asia Pacific) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Europe-Africa-Middle East) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH7010 PPE+PS Noryl* NH7010 resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight parts.. |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL NH7010 PPE+PS (Asia Pacific) High heat, Non halogenated flame retardant Noryl product |
|||
Vicat Softening Point | 161 °C | 322 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL EXNL1285 PPE+PS (Europe-Africa-Middle East) Noryl* EXNL1285 Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Vicat Softening Point | 161 °C | 322 °F | temperature A; ISO 306 |
Lubrizol ESTALOC® T5160 Ether-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Vicat Softening Point | 161 °C @Load 1.00 kg, Thickness 3.17 mm |
322 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1527 |
Diamond Polymers DIAMALOY 627 PC/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 161 °C | 322 °F | under 1 daN; ASTM D1525 |
Arkema Group Pebax® 6333 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Vicat Softening Point | 161 °C | 322 °F | 50°C/hr; 50N |
Arkema Group Pebax® 6333 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 63 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
Vicat Softening Point | 161 °C | 322 °F | 50 N; ISO 306 |
Azoty Tarnow™ TARNOFORM 300 GF5 POM 26% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Vicat Softening Point | 161 °C | 322 °F | 50 N; ISO 306 |
Azoty Tarnow™ TARNOFORM 411 POM Easy flowing, internally strengthened grade for injection molding of thin walled parts of very high mechanical requirements.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |