SABIC Innovative Plastics NORYL EXNL1285 PPE+PS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL EXNL1285 PPE+PS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Noryl* EXNL1285 Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; this grade has been developed for fluid engineering applications where higher static stiffness is required.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Water Absorption at Saturation 0.20 %
0.20 %
ISO 62
Melt Index of Compound 20 g/10 min

@Load 10.0 kg,
Temperature 300 °C
20 g/10 min

@Load 22.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 155 MPa
22500 psi
5 mm/min; ISO 527
Elongation at Break 1.8 %
1.8 %
5 mm/min; ISO 527
Tensile Modulus 11.3 GPa
1640 ksi
1 mm/min; ISO 527
Flexural Yield Strength 195 MPa
28300 psi
2 mm/min; ISO 178
Flexural Modulus 9.50 GPa
1380 ksi
2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Vicat Softening Point 161 °C
322 °F
Rate B/120; ISO 306