Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.500 GPa | 72.5 ksi | ISO 178 |
Polimeri Europa Flexirene® MR 50 A Linear Low Density Polyethylene Flexirene MR 50 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity... |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | ISO 178 |
Polimeri Europa Flexirene® MR 50 U Linear Low Density Polyethylene Flexirene MR 50 U is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 U are characterized by optimum rigidity... |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | ISO 178 |
Polimeri Europa Flexirene® MR 56 A Linear Low Density Polyethylene Flexirene MR 56 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MR 50 A are characterized by optimum rigidity... |
|||
Flexural Modulus | 0.500 GPa @Temperature 90.0 °C |
72.5 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilitop BT N Unfilled, Nucleated PBT Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent.. |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | ASTM D790 |
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Flexural Modulus | >= 0.500 GPa | >= 72.5 ksi | ASTM D1238 |
NIZHNEKAMSKNEFTEKHIM PE 4025W (25425) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 0.500 - 0.500 GPa @Temperature 90.0 - 90.0 °C |
72.5 - 72.5 ksi @Temperature 194 - 194 °F |
Average value: 0.500 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | ASTM D790 |
NOVA Chemicals Sclair® 96A HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, excellent stretchability, superior strength, gel free.Applications: Oriented tapes for industrial woven bags and tarpaulins, monoaxial oriented films.Data provide.. |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | ASTM D790 |
NOVA Chemicals Sclair® 96A-UV8D HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, excellent stretchability, superior strength, gel free, excellent UV resistance.Applications: Oriented tapes for industrial woven bags and tarpaulins, monoaxial or.. |
|||
Flexural Modulus | 0.500 GPa @Temperature 120 °C |
72.5 ksi @Temperature 248 °F |
ASTM D790 |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | ASTM D790 |
Reliance Industries Reclair ER-19 Reclair ER-19 is a Octene Conomer based medium density Polyethylene grade designed for Rotational Molding applications with optimum loading of UV Stabilizer. Processing is similar to Butene grades... |
|||
Flexural Modulus | 0.500 GPa @Temperature 65.0 °C |
72.5 ksi @Temperature 149 °F |
ASTM D790 |
BASF Capron® 8200 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 0.500 GPa @Temperature 65.0 °C |
72.5 ksi @Temperature 149 °F |
ASTM D790 |
BASF Capron® 8202 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | ASTM D790 |
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE. |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | ASTM D790 |
Covestro Bayflex® 110 RIM-LITE Polyurethane Elastomeric RIM, 13% Mineral Filled, MDI-based 2-Component Liquid System Contains 10% calcium silicate and 3% glass microspheres.0.15 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, .. |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | ISO 178 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | After conditioning at 23°C and 50% RH; ISO 178 |
Arkema Group Orgalloy® LE 60LMXV Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | Dry; ISO 178 |
Arkema Group Orgalloy® LT 4060 ES Polyamide Alloy Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | Dry; ISO 178 |
Arkema Group Orgalloy® LT 4060 Polyamide Alloy Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | SAE J949 |
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness) AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | ASTM D790 |
Buckeye Polymers BP Flex A9505 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Flexural Modulus | 0.500 GPa @Temperature 65.0 °C |
72.5 ksi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Flexural Modulus | 0.500 GPa @Temperature 65.0 °C |
72.5 ksi @Temperature 149 °F |
ASTM Test |
BASF Ultramid® 8202 PA6 (Dry) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | After conditioning at 23°C and 50% RH; ISO 178 |
Arkema Group Orgalloy® LT 5050 Polyamide Alloy Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | ASTM D790 |
Buckeye Polymers BP Flex D0853 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Flexural Modulus | 0.500 - 4.83 GPa | 72.5 - 700 ksi | Average value: 1.19 GPa Grade Count:63 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | ASTM D790 |
Buckeye Polymers BP Flex D4507 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Flexural Modulus | 0.500 GPa @Temperature 23.0 °C |
72.5 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET
(Unverified Data**) Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont |
|||
Flexural Modulus | 0.500 GPa | 72.5 ksi | After conditioning at 23°C and 50% RH; ISO 178 |
Arkema Group Orgalloy® LT 5050 ES Polyamide Alloy Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group |