Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Quadrant Engineering Plastics Products
Trade Name TIVAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic flow
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Water Absorption <= 0.010 %
<= 0.010 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.010 %
<= 0.010 %
Immersion; ASTM D570(2)
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Tensile Modulus 0.421 GPa
61.0 ksi
ASTM D638
Flexural Strength 22.1 MPa
3200 psi
ASTM D790
Flexural Modulus 0.500 GPa
72.5 ksi
ASTM D790
Compressive Strength 20.7 MPa
3000 psi
10% Def.; ASTM D695
Compressive Modulus 0.483 GPa
70.0 ksi
ASTM D695
Izod Impact, Notched NB
NB
ASTM D256 Type A
Coefficient of Friction, Dynamic 0.12
0.12
Dry vs. Steel; QTM55007
Sand Slurry 8.0
8.0
1018 Steel = 100
Limiting Pressure Velocity 0.140 MPa-m/sec
4000 psi-ft/min
4:1 safety factor; QTM 55007
Thermal Properties Metric English Comments
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.409 W/m-K
2.84 BTU-in/hr-ft²-°F
Melting Point 135 °C
275 °F
Crystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 82.2 °C
180 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 46.7 °C
116 °F
ASTM D648
Flammability, UL94 HB
HB
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+15 ohm
>= 1.00e+15 ohm
ASTM D257
Dielectric Constant 2.3

@Frequency 1e+6 Hz
2.3

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 90.6 kV/mm
2300 kV/in
Short Term; ASTM D149
Dissipation Factor 0.00050

@Frequency 1e+6 Hz
0.00050

@Frequency 1e+6 Hz
ASTM D150
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA No
No
NSF No
No
USDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative No
No
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Unacceptable
Unacceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Limited
Limited
Descriptive Properties Value Comments
Machinability 3
1-10, 1=Easier to Machine