Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical LG709W ABS, Low Gloss, Heat Resistance Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Pilllars, Etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG.. |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN1006FL PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided.. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Gromax PBT 1100-211D Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Gromax PBT 1100-211S Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat ResistanceApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP1000MD PC, Light Diffusion Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP1000SW PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: Keypad for Mobile Phone, Automotive (Interior)CAS: 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® FD-1122 PC, FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NE-1050 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® LX-0935 S ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9300HF ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Samyang Tribit® 1503 Polybutylene Terephthalate Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid.. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Samyang Triloy® 210NHF Polymer Alloy, Flame Retardancy (Non-Halogen) Excellent impact, formability and weather resistance.210NHF is a flame retardant (non-halogen) grade.Applications: LCD TV Rear Cover (high flow)Information provided by Samyang. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Samyang Trirex® 3015NF Polycarbonate, Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3015NF is a flame retardant grade.Applications: Mobile Phone - battery caseInformation.. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | ASTM D790 |
Samyang Trirex® 3025N1 Polycarbonate, Flame Retardant TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® UF-1013 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.25 GPa | 327 ksi | ASTM D-790 |
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret.. |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron HR-59 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron HR-60 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Flexural Modulus | 2.26 GPa @Thickness 6.40 mm |
327 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IM-11GM ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Flexural Modulus | 2.26 GPa | 327 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1021 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP1000ML PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |