Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.15 - 2.40 GPa | 312 - 348 ksi | ASTM D790 |
Prodways PLASTCure Model 300 3D Printing Polymer Good mechanical properties.Broad range of dental model applications.Information provided by Genistar. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Asia Pacific) Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Asia Pacific) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL5302 PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML3400 PC (Europe-Africa-Middle East) LEXAN ML3400 is a medium viscosity, impact modified grade with improved chemical resistance. It passes the British Standard 2495 and 5361 solvent tests. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXE9925A PC (Asia Pacific) Illuminate / edge glow color effect grade of Lexan 9925A. 9925A is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR .. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
SABIC Innovative Plastics Lexan® ML1665 PC (Asia Pacific) |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2mm/min; ASTM D790 |
Kingfa FRHIPS-220 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
Hannam Chemical Hanalac 775 ABS, Extrusion Grade Increased chemical resistance. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors,.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® HX3091HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS LNP* STAT-LOY* N30009 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL PX1005X PPE+HIPS (Asia Pacific) PPE+PS 80deg.C FR V-0 |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Asia Pacific) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the A.. |
|||
Flexural Modulus | 2.15 GPa @Thickness 3.17 mm |
312 ksi @Thickness 0.125 in |
|
TPI Porene® ABS-GA803 High Gloss, UV Resistant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D 790 |
Cossa Polimeri ESTADIENE 3015 MT Acrylonitrile Butadiene Styrene ABSMedium thermal resistance, high impact resistance at low temperature, good melt flow rate, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | chs 0.05 in/min; tangent; ASTM D790 |
Diamond Polymers NPP 808 C3 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2.6 mm/min; ASTM D790 |
BLUESTAR LXS 110 PPE-PS Typical Applications: Electrical partsFire RatedInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
Tipco Tipcolene® FPC 30 PPC - 30% Calcium Carbonate Reinforced Polypropylene Copolymer 30% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL 115 PPE+HIPS (Asia Pacific) PPE+PS, 115 oC HDT |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
Teknor Apex Sinpolene CPP1040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 40% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F.. |