Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP 808 C3 TDS Polycarbonate Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Diamond Polymers NPP 808 C3 TDS Polycarbonate Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Water Absorption 0.35 %
<br>@Temperature 23.0 °C
0.35 %
<br>@Temperature 73.4 °F
Equilibrium; ASTM D570
0.15 %
<br>@Temperature 23.0 °C,<br> Time 86400 sec
0.15 %
<br>@Temperature 73.4 °F,<br> Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 4.5 g/10 min
<br>@Load 5.00 kg,<br> Temperature 200 °C
4.5 g/10 min
<br>@Load 11.0 lb,<br> Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.6 MPa
7920 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 233 %
233 %
ASTM D638
Flexural Modulus 2.15 GPa
312 ksi
chs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched NB
<br>@Thickness 3.17 mm,<br> Temperature 23.0 °C
NB
<br>@Thickness 0.125 in,<br> Temperature 73.4 °F
reverse notched; ASTM D256
Gardner Impact >= 36.2 J
<br>@Temperature 23.0 °C
>= 26.7 ft-lb
<br>@Temperature 73.4 °F
ASTM D5420
>= 36.2 J
<br>@Temperature -17.8 °C
>= 26.7 ft-lb
<br>@Temperature -0.0400 °F
ASTM D5420
>= 36.2 J
<br>@Temperature -28.9 °C
>= 26.7 ft-lb
<br>@Temperature -20.0 °F
ASTM D5420
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 90 %
90 %
ASTM D1003