Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.10 GPa | 305 ksi | |
Plastcom SLOVALEN PC 81 T 15 PP, 15% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 15% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitur.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Asia Pacific) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Flexural Modulus | 2.10 GPa @Temperature 23.0 °C |
305 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT
(Unverified Data**) Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | ASTM D790 |
Gichem GILAC E200 Acrylonitrile Butadiene Styrene
(discontinued **) ABS medium fluidity, excellent resilience. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 2mm/min; ASTM D790 |
3M Dyneon™ PVDF 1012/1001 Polyvinylidene Fluoride
(discontinued **) High molecular weight grade PVDFPowder gradeExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent strength and dimensional stabilityInf.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 15 mm/min; ASTM D790 |
LG Chemical 65IH HIPS High impact, Extrusion, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food tray.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL V090 PPE+HIPS (Europe-Africa-Middle East) NORYL V090 is an unfilled, flame retardant material with a Vicat B/120 of 95 °C according ISO 306. NORYL V090 is V0 at 2.0 mm and V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 47.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp ZP003 PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZP003 is a compound based on PPE + PS Blend resin containing PTFE, Silicone. Added features include Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | ASTM D790 |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | ASTM D790 |
Techmer ES Luriblend® POM CO E TL20 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Good Wear Resistance and CopolymerProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | ASTM D790 |
Techmer ES Luriblend® POM CO TL20 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerUL File Number: E157318Information provided by TP Composit.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp FX05032 PE (Europe-Africa-Middle East) LNP* THERMOCOMP* FX05032 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added features include : Foaming Agent for Polyolefins.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 3 points; ISO 178 |
Styron Pulse® A35-105 PC/ABS PULSE™ A35-105 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature.Information provided by DowThis product line was spun off f.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL HH180 PPE+PS Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Asia Pacific) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX1005X PPE+HIPS (Europe-Africa-Middle East) Noryl PX1005X is an unfilled, low heat resistance, halogen free (according VDE/DIN 472 part 813) flame retardant material. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 3 points and 2 mm/min; ISO 178 |
Styron Pulse® 920 MG PC/ABS An inherently matt medium heat, medium impact PC/ABS resin, PULSE™ 920 MG is designed for interior automotive applications where a matt aesthetic is required.Information provided by DowThis pro.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | ISO 178 |
SABIC Innovative Plastics NORYL EM6100 PPE+PS PPE+PS blend. Unfilled. Good balance of flow/heat/impact. Dimensional stability. Paint adhesion. Suitable for the automotive interior market: HVAC housings, radio components. MS-DB424, WSB-M4D844-A9.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | ISO 178 |
Total Polystyrene Impact 6540 Easy Flow Impact Polystyrene POLYSTYRENE IMPACT 6540 is an easy flowing, high impact polystyrene with a good balance of mechanical and thermal properties. This resin combines physical properties such as the flow necessary for .. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 1.3 mm/min, 50 mm span, method 1, tangent; ASTM D790 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | 2 mm/min; ISO 178 |
Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 152 Polypropylene, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | ASTM D790 |
Ashley Polymers Ashlene® 1021T Polycarbonate A high flow, high impact resin.Data provided by the manufacturer |
|||
Flexural Modulus | 2.10 GPa | 305 ksi | ASTM D790 |
Ashley Polymers Ashlene® 256 PPO A general purpose grade with good heat resistance and impact strength. Other properties include dimensional stability and moisture resistance.Data provided by the manufacturer |