Total Polystyrene Impact 6540 Easy Flow Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Total Atofina
Trade Name Polystyrene Impact
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Total Polystyrene Impact 6540 Easy Flow Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
POLYSTYRENE IMPACT 6540 is an easy flowing, high impact polystyrene with a good balance of mechanical and thermal properties. This resin combines physical properties such as the flow necessary for large or complex moldings, the impact resistance for good mechanical properties in thin wall sections and good thermal properties for articles subjected to elevated temperatures in use. The combination of properties also offers high productivity.Applications POLYSTYRENE IMPACT 6540 satisfies the requirements of a wide range of molding applications. Toys, television housing, food packaging, refrigerator, computer keyboards, office equipment, household items...Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
Melt Flow 11.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
11.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133 H
Mechanical Properties Metric English Comments
Hardness, Rockwell R 78
78
ISO 2039-2
Tensile Strength at Break 20.0 MPa
2900 psi
ISO 527-2
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-2
Elongation at Break >= 45 %
>= 45 %
ISO 527-2
Flexural Modulus 2.10 GPa
305 ksi
ISO 178
Izod Impact, Notched (ISO) 9.50 kJ/m²
4.52 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear 91.0 µm/m-°C
50.6 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
unannealed; ISO 75-2A
80.0 °C
176 °F
annealed; ISO 75-2A
Vicat Softening Point 83.0 °C

@Load 5.10 kg
181 °F

@Load 11.2 lb
50°C per hour; ISO 306B50
92.0 °C

@Load 1.02 kg
198 °F

@Load 2.25 lb
50°C per hour; ISO 306A50
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO IEC 93
Dielectric Strength 150 kV/mm
3810 kV/in