Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Luriblend® POM CO TL20 Acetal

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, PTFE Filled
Manufacturer Techmer ES
Trade Name Luriblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® POM CO TL20 Acetal.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerUL File Number: E157318Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Water Absorption 0.15 %

@Time 86400 sec
0.15 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.020 cm/cm

@Thickness 3.17 mm
0.020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79
79
ASTM D785
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Flexural Strength 67.6 MPa
9800 psi
ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 99.0 µm/m-°C
55.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C
210 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Strength 19.7 kV/mm
500 kV/in
Method A (Short-Time); ASTM D149